Effect of Cr on microstructural evolution of aluminized fourth generation Ni-base single crystal superalloys

被引:21
|
作者
Suzuki, A. S. [1 ]
Kawagishi, K. [1 ]
Yokokawa, T. [1 ]
Harada, H. [1 ]
机构
[1] Natl Inst Mat Sci, Environm & Energy Mat Div, High Temp Mat Unit, Tsukuba, Ibaraki 3050047, Japan
来源
SURFACE & COATINGS TECHNOLOGY | 2012年 / 206卷 / 11-12期
关键词
Coating; Aluminizing; SRZ; Microstructure; Ni-base superalloys; THERMAL BARRIER COATINGS; OXIDATION BEHAVIOR; PLATINUM; ZONE;
D O I
10.1016/j.surfcoat.2011.11.029
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
An effect of Cr on microstructural evolution of aluminized fourth generation Ni-base single crystal superalloys was investigated. Aluminized fourth generation alloys, having different amounts of Cr in substrates, were examined at 1100 degrees C up to 300 h. After aluminizing, all alloys exhibited similar phase constitutions, however, they showed distinctive morphologies of secondary reaction zones (SRZs): an alloy containing the highest Cr content developed continuous SFZs under an inter-diffusion zone (IDZ), whereas the other alloys hardly developed SRZ formation. The highest Cr containing alloy particularly exhibited higher coverage of SRZ after aluminizing, and this suggests higher Cr in substrate encourages SRZ formation. All alloys developed more SRZ formation after 300 h, and higher Cr containing alloys precipitated more topologically close-packed (TCP) phases in substrate. All alloys demonstrated increases of SRZ coverage, whereas penetration depth of SRZ in each alloy was not significantly different after 300 h. Higher Cr containing alloys precipitated TCP phases in substrate after 300 h, and this prevents further growth of SRZ. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:2769 / 2773
页数:5
相关论文
共 50 条
  • [1] Effect of cobalt on microstructural parameters and mechanical properties of Ni-base single crystal superalloys
    Suzuki, Takanobu
    Yokokawa, Tadaharu
    Kobayashi, Toshiharu
    Koizumi, Yutaka
    Harada, Hiroshi
    Imai, Hachiro
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2007, 71 (02) : 233 - 238
  • [2] INFLUENCE OF CRYSTALLOGRAPHIC ORIENTATION ON CREEP BEHAVIOR OF ALUMINIZED NI-BASE SINGLE CRYSTAL SUPERALLOYS
    Latief, F. H.
    Kakehi, K.
    Murakami, H.
    Kasai, K.
    SUPERALLOYS 2012, 2012, : 311 - 320
  • [3] Secondary Reaction Zone Formations in Pt-Aluminised fourth generation Ni-base single crystal superalloys
    Suzuki, A. S.
    Rae, C. M. F.
    Hobbs, R. A.
    Murakami, H.
    EURO SUPERALLOYS 2010, 2011, 278 : 78 - +
  • [4] Effects of Re content and crystallographic orientation on creep behavior of aluminized Ni-base single crystal superalloys
    Latief, Fahamsyah H.
    Kakehi, Koji
    MATERIALS & DESIGN, 2013, 49 : 485 - 492
  • [5] On Shear Testing of Single Crystal Ni-Base Superalloys
    Eggeler, G.
    Wieczorek, N.
    Fox, F.
    Berglund, S.
    Burger, D.
    Dlouhy, A.
    Wollgramm, P.
    Neuking, K.
    Schreuer, J.
    Jacome, L. Agudo
    Gao, S.
    Hartmaier, A.
    Laplanche, G.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (09): : 3951 - 3962
  • [6] Microstructural aspects of fatigue in Ni-base superalloys
    Antolovich, Stephen D.
    PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 2015, 373 (2038):
  • [7] Influence of Ru on the Microstructure of Ni-base Single Crystal Superalloys
    Sun, Fei
    Zhang, Jianxin
    EMERGING FOCUS ON ADVANCED MATERIALS, PTS 1 AND 2, 2011, 306-307 : 562 - 571
  • [8] Sulfur embrittlement on γ/γ′ interface of Ni-base single crystal superalloys
    Chen, K
    Zhao, LR
    Tse, JS
    ACTA MATERIALIA, 2003, 51 (04) : 1079 - 1086
  • [9] Predicting freckle formation in single crystal Ni-base superalloys
    S. Tin
    T. M. Pollock
    Journal of Materials Science, 2004, 39 : 7199 - 7205
  • [10] Effect of minor alloying additions on the solidification of single-crystal Ni-base superalloys
    Cutler, E. R.
    Wasson, A. J.
    Fuchs, G. E.
    JOURNAL OF CRYSTAL GROWTH, 2009, 311 (14) : 3753 - 3760