Defect evolution of 409L stainless steel in high-speed TIG welding

被引:16
作者
Feng, Chao [1 ,2 ]
Qin, Guoliang [1 ,2 ]
Meng, Xiangmeng [1 ,2 ]
Geng, Peihao [1 ,2 ]
机构
[1] Shandong Univ, Minist Educ, Key Lab Liquid Solid Struct Evolut & Proc Mat, Jinan 250061, Shandong, Peoples R China
[2] Shandong Univ, Inst Mat Joining, Jinan, Shandong, Peoples R China
基金
中国国家自然科学基金;
关键词
Flow; measurement; simulation; high-speed; processing; undercut; humping; defect; manufacturing; modeling; geometry; MOLTEN POOL BEHAVIOR; BEAD HUMP FORMATION; PROCESS PARAMETERS; FLUID-FLOW; ARC; GAS; QUALITY; GTAW;
D O I
10.1080/10426914.2020.1711925
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The undercut and humping weld defects in high-speed tungsten inert gas (TIG) welding deteriorate the mechanical properties of the weld, which limit the improvement of modern manufacturing. Based on the heat and mass transfer in the molten pool, the geometry of the molten pool and depression region and the maximum backward velocity of the lateral channel were emphatically analyzed as the heat input being retained to be basically consistent at different welding speeds. As the welding speed increases from 1.0 m/min to 3.0 m/min, the maximum backward velocity of the lateral channel increases from 0.31 m/s to 0.57 m/s, which aggravates the undercut defect. The undercut defect initially appears in the weld at 1.5 m/min and becomes more serious with increasing welding speed. Additionally, the length of the depression region of the molten pool shows an increasing trend. The humping weld defects are first observed in the weld at 2.8 m/min, and the length of the depression region exceeds 3.6 mm. These findings prove the complicated behavior in the molten pool due to the complex thermo-mechanical coupling effect, and also provide a possibility to obtain sound welds efficiently by selecting suitable welding parameters in high-speed TIG welding process.
引用
收藏
页码:179 / 186
页数:8
相关论文
共 35 条
[1]   Hybrid laser arc welding: State-of-art review [J].
Acherjee, Bappa .
OPTICS AND LASER TECHNOLOGY, 2018, 99 :60-71
[2]   GTA pulsed current welding of thin sheets of SS304 producing superior quality of joint at high welding speed [J].
Agrawal, B. P. ;
Chauhan, Ankit Kumar ;
Kumar, Ravindra ;
Anant, Ramkishor ;
Kumar, Sudhir .
JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2017, 39 (11) :4667-4675
[3]  
BRADSTREET BJ, 1968, WELD J, V47, pS314
[4]   Understanding bead hump formation in gas metal arc welding using a numerical simulation [J].
Cho, Min Hyun ;
Farson, Dave F. .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2007, 38 (02) :305-319
[5]   Effect of welding speed on microstructures, mechanical properties and corrosion behavior of GTA-welded AISI 201 stainless steel sheets [J].
Chuaiphan, Wichan ;
Srijaroenpramong, Loeshpahn .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2014, 214 (02) :402-408
[6]   Effects of process parameters on the quality aspects of weld-bead in laser welding of NiTinol sheets [J].
Datta, Susmita ;
Raza, Mohammad Shahid ;
Saha, Partha ;
Pratihar, D. K. .
MATERIALS AND MANUFACTURING PROCESSES, 2019, 34 (06) :648-659
[7]   Heat transfer and fluid flow in a partially or fully penetrated weld pool in gas tungsten arc welding [J].
Fan, HG ;
Tsai, HL ;
Na, SJ .
INTERNATIONAL JOURNAL OF HEAT AND MASS TRANSFER, 2001, 44 (02) :417-428
[8]  
FUERSCHBACH PW, 1991, WELD J, V70, pS287
[9]   Effects of process parameters on weld bead defects in oscillating laser-GMA hybrid welding of lap joints [J].
Gao, X. S. ;
Wu, C. S. ;
Goecke, S. F. ;
Kuegler, H. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 93 (5-8) :1877-1892
[10]   Arc characteristics and behaviour of metal transfer in pulsed current GMA welding of stainless steel [J].
Ghosh, P. K. ;
Dorn, Lutz ;
Kulkarni, Shrirang ;
Hofmann, F. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (03) :1262-1274