Incorporation of PVP into PEG/PMMA based binder system to minimize void nucleation

被引:5
作者
Hayat, Muhammad Dilawer [1 ]
Li, Tao [2 ]
Cao, Peng [1 ]
机构
[1] Univ Auckland, Dept Chem & Mat Engn, Auckland 1142, New Zealand
[2] Singapore Inst Mfg Engn SIMTech, Singapore, Singapore
关键词
PEG/PMMA; Void nucleation; Metal injection molding; Polymer crystallization; POLY(ETHYLENE GLYCOL); BEHAVIOR; CRYSTALLIZATION; PYRROLIDONE); WATER; DEGRADATION; TEMPERATURE; DEFECTS; POLYMER; BLENDS;
D O I
10.1016/j.matdes.2015.08.131
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In spite of its great potential, the polyethylene glycol (PEG) and polymethyl methacrylate (PMMA) binder system was found susceptible to void nucleation, as the rigid PMMA chains hinder PEG volumetric shrinkage upon cooling. We previously reported that this void formation could be minimized by either using a higher cooling rate or by incorporating a crystallization inhibitor in the binder system. In this paper, efforts have been made to increase the workability of this binder system for conventional metal injection molding (MIM) by adding the crystallization inhibitor, polyvinylpyrrolidone (PVP). Differential scanning calorimetry (DSC), rheological property measurements, solvent and thermal debinding behavior, and fracture surface analysis of the molded samples were performed. Incorporation of PVP into the PEG/PMMA binder system is successful in that high quality void-free MIM components have been produced while maintaining the clean nature of the PEG/PMMA binder system. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:932 / 938
页数:7
相关论文
共 34 条
[1]   Electrical conductivity and dielectric behavior of some poly(alkyl methacrylate)s/polyvinylpyrrolidone blends [J].
Abd-El-Messieh, SL ;
Naguib, HF .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2005, 44 (8-9) :1591-1606
[2]  
[Anonymous], POL POL BROCH
[3]  
ASTM, 2013, STAND SPEC MET INJ M
[4]  
Cao M.Y., 1992, POWD MET WORLD CAPMI
[5]  
Chen G., 2012, POWDER INJECTION MOU, V6, P83
[6]   Debinding behaviour of a water soluble PEG/PMMA binder for Ti metal injection moulding [J].
Chen, Gang ;
Cao, Peng ;
Wen, Guian ;
Edmonds, Neil .
MATERIALS CHEMISTRY AND PHYSICS, 2013, 139 (2-3) :557-565
[7]   Crystallization behavior and hydrophilicity of poly(vinylidene fluoride)/poly(methyl methacrylate)/poly(vinyl pyrrolidone) ternary blends [J].
Cheng, Jing ;
Wang, Shichao ;
Chen, Shuangjun ;
Zhang, Jun ;
Wang, Xiaolin .
POLYMER INTERNATIONAL, 2012, 61 (03) :477-484
[8]  
Chuankrerkkul N, 2008, CHIANG MAI J SCI, V35, P188
[9]   Solid state NMR study of poly(methyl methacrylate) polyvinylpyrrolidone blends [J].
da Silva, EP ;
Tavares, MIB .
POLYMER BULLETIN, 1998, 41 (03) :307-310
[10]   Molecular and nanoscale factors governing pressure-sensitive adhesion strength of viscoelastic polymers [J].
Feldstein, Mikhail M. ;
Siegel, Ronald A. .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2012, 50 (11) :739-772