A new and rapid process for production of solution-derived (Pb,La)(Zr,Ti)O-3 thin films and powders

被引:26
作者
Boyle, TJ
AlShareef, HN
机构
[1] Sandia National Laboratories, Albuquerque, NM 87106
基金
美国能源部;
关键词
D O I
10.1023/A:1018520132376
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A simple and rapid process for synthesizing (Pb,La)(Zr,Ti)O-3 (PZT, PLZT, and PLT) precursor solutions has been developed. This process, termed the ''basic route to PLZT'' (or BRP) process, offers several advantages over standard methods, including rapid solution synthesis (<10 min), use of commercially available materials, film production under ambient conditions, ease of lanthanum dissolution at high concentrations (<1 min), and no heating requirements during solution synthesis. The PLZT precursor solution synthesis involves dissolution of lead acetate (or acetyl acetate) in pyridine followed by addition of a pre-dissolved mixture of titanium and zirconium iso-propoxide in toluene. The lanthanum source can then be added and, depending on the precursor, total synthesis time was <10 min. The preferred lanthanum starting material is a highly soluble bis(isopropyl)aryloxide complex; however, this compound is extremely air and water sensitive. The compositions investigated in this study include PZT 40/60, PLZT 3130/70, 5/30/70, and 10/40/60, and PLT films with 10-20 mol% La. All films were crystallized at 650 degrees C and exhibit ferroelectric properties comparable to films produced by other techniques which require higher crystallization temperatures.
引用
收藏
页码:2263 / 2266
页数:4
相关论文
共 12 条
[1]   H-1 AND C-13 NMR INVESTIGATIONS OF PB(ZR,TI)O3 THIN-FILM PRECURSOR SOLUTIONS [J].
ASSINK, RA ;
SCHWARTZ, RW .
CHEMISTRY OF MATERIALS, 1993, 5 (04) :511-517
[2]   SYNTHESIS, PROPERTIES, AND X-RAY STRUCTURES OF THE LANTHANIDE ETA-6-ARENE-BRIDGED ARYLOXIDE DIMERS LN2(O-2,6-I-PR2C6H3)6 AND THEIR LEWIS BASE ADDUCTS LN(O-2,6-I-PR2C6H3)3(THF)2 (LN=PR, ND, SM, GD, ER, YB, LU) [J].
BARNHART, DM ;
CLARK, DL ;
GORDON, JC ;
HUFFMAN, JC ;
VINCENT, RL ;
WATKIN, JG ;
ZWICK, BD .
INORGANIC CHEMISTRY, 1994, 33 (16) :3487-3497
[3]  
Budd K. D., 1985, British Ceramic Proceedings, P107
[4]   AMMONIACAL SYNTHESIS OF LANTHANUM ARYLOXIDE COMPLEXES AND OBSERVATION OF A UNIQUE INTERCONVERSION BETWEEN OXYGEN-BRIDGED AND ETA-ARENE-BRIDGED DIMERIC SPECIES - X-RAY CRYSTAL-STRUCTURES OF LA-2(OAR)(6)(NH3)(N) (N=0, 2), LA(OAR)(3)(NH3)(4), AND LA(OAR)(3)(THF)(2) (AR=2,6-I-PR2C6H3) [J].
BUTCHER, RJ ;
CLARK, DL ;
GRUMBINE, SK ;
VINCENTHOLLIS, RL ;
SCOTT, BL ;
WATKIN, JG .
INORGANIC CHEMISTRY, 1995, 34 (22) :5468-5476
[5]  
DIMOS D, 1995, COMMUNICATION
[6]   PREPARATION OF FERROELECTRIC PZT FILMS BY THERMAL-DECOMPOSITION OF ORGANOMETALLIC COMPOUNDS [J].
FUKUSHIMA, J ;
KODAIRA, K ;
MATSUSHITA, T .
JOURNAL OF MATERIALS SCIENCE, 1984, 19 (02) :595-598
[7]   PLZT THIN-FILMS PREPARED FROM ACETATE PRECURSORS [J].
HAERTLING, GH .
FERROELECTRICS, 1991, 116 (1-2) :51-63
[8]  
SCHWARTZ RW, 1992, MATER RES SOC S P, V243, P245
[9]   Properties of ferroelectric (Pb,La)(Zr,Ti)O-3 thin films by MOCVD [J].
Shimizu, M ;
Fujisawa, H ;
Shiosaki, T .
INTEGRATED FERROELECTRICS, 1995, 10 (1-4) :23-30
[10]  
TEOWEE G, 1992, MATER RES SOC S P, V243, P255