Effect of ball milling time on the thermoelectric properties of p-type (Bi,Sb)2Te3

被引:124
作者
Son, J. H. [1 ,2 ]
Oh, M. W. [1 ]
Kim, B. S. [1 ]
Park, S. D. [1 ]
Min, B. K. [1 ]
Kim, M. H. [2 ]
Lee, H. W. [1 ]
机构
[1] Korea Electrotechnol Res Inst, Fundamental & Creat Res Div, Changwon Si 642120, South Korea
[2] Changwon Natl Univ, Dept Convergence Mat Sci & Engn, Chang Won 641773, South Korea
基金
新加坡国家研究基金会;
关键词
Thermoelectric properties; Ball milling; (Bi; Sb)(2)Te-3; Thermal conductivity; Bi2Te3; ANTISITE DEFECTS; DOPED BI2TE3; CRYSTALS; SEMICONDUCTOR; PERFORMANCE; ALLOYS;
D O I
10.1016/j.jallcom.2013.03.062
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
P-type (Bi,Sb)(2)Te-3 compounds were fabricated with high energy ball-milled powder and their thermoelectric properties were investigated as a function of the ball milling time. The fine grain sizes were confirmed with the X-ray analysis and the microscopy images in the samples fabricated with powders from long ball milling time. The values of the lattice thermal conductivity of the samples at high temperature show smaller values for long milling time (>24h) than those for short time, resulted from the finer grain sizes of the samples. As well as the microstructural change, the Seebeck coefficient and the electrical resistivity of the compounds were significantly altered with the ball milling time. The carrier concentration was dramatically increased in the samples after 24 h milling, which was attributed to the formation of the antisite defects introduced by the accumulated thermal energy. The formation of antisite defects may be also promoted by the unintentional Fe doping from jars and balls. The highest value of ZT = 1.14 was achieved at 323 K for the samples with 10 h. The temperature where the value of ZT was maximized and the values of ZT was varied with the ball milling time, which implies that the ball milling time should be carefully optimized for the suitable application of this compounds. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:168 / 174
页数:7
相关论文
共 28 条
[1]   ELECTRONEGATIVITY VALUES FROM THERMOCHEMICAL DATA [J].
ALLRED, AL .
JOURNAL OF INORGANIC & NUCLEAR CHEMISTRY, 1961, 17 (3-4) :215-221
[2]   Antisite defects of Bi2Te3 thin films [J].
Cho, SL ;
Kim, Y ;
DiVenere, A ;
Wong, GK ;
Ketterson, JB ;
Meyer, JR .
APPLIED PHYSICS LETTERS, 1999, 75 (10) :1401-1403
[3]   Effect of Ag or Sb addition on the thermoelectric properties of PbTe [J].
Dow, H. S. ;
Oh, M. W. ;
Kim, B. S. ;
Park, S. D. ;
Min, B. K. ;
Lee, H. W. ;
Wee, D. M. .
JOURNAL OF APPLIED PHYSICS, 2010, 108 (11)
[4]   Estimation of the thermal band gap of a semiconductor from Seebeck measurements [J].
Goldsmid, HJ ;
Sharp, JW .
JOURNAL OF ELECTRONIC MATERIALS, 1999, 28 (07) :869-872
[5]   First-principles density functional theory study of native point defects in Bi2Te3 [J].
Hashibon, Adham ;
Elsaesser, Christian .
PHYSICAL REVIEW B, 2011, 84 (14)
[6]   ENERGY FORMATION OF ANTISITE DEFECTS IN DOPED SB2TE3 AND BI2TE3 CRYSTALS [J].
HORAK, J ;
CERMAK, K ;
KOUDELKA, L .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1986, 47 (08) :805-809
[7]   Thermoelectric power and Shubnikov-de Haas effect in magnetic impurity-doped Bi2Te3 and Bi2Se3 [J].
Kulbachinskii, VA ;
Kaminskii, AY ;
Kytin, VG ;
de Visser, A .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2004, 272 :1991-1992
[8]   Ferromagnetism in new diluted magnetic semiconductor Bi2-xFexTe3 [J].
Kulbachinskii, VA ;
Kaminskii, AY ;
Kindo, K ;
Narumi, Y ;
Suga, K ;
Lostak, P ;
Svanda, P .
PHYSICA B-CONDENSED MATTER, 2002, 311 (3-4) :292-297
[9]   Thermoelectric transport properties of bismuth telluride bulk materials fabricated by ball milling and spark plasma sintering [J].
Kuo, Chia-Hung ;
Hwang, Chii-Shyang ;
Jeng, Ming-Shan ;
Su, Wei-Sheng ;
Chou, Ya-Wen ;
Ku, Jie-Ren .
JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 496 (1-2) :687-690
[10]   DER EINFLUSS VON UBERSCHUSSIGEM ANTISTRUKTURELLEM BI AUF DIE WARMELEITFAHIGKEIT DES KRISTALLGITTERS VON BI2TE3 BI2TE3-SB2TE3 UND BI2TE3-BI2S3 MIT JODBEIMISCHUNG [J].
KUTASOV, VA ;
SMIRNOV, IA .
PHYSICA STATUS SOLIDI, 1966, 18 (01) :479-&