Fatigue and fracture characteristics of a fine-grained (Mg,Y)-PSZ zirconia ceramic

被引:6
|
作者
Fernàndez, R
Meschke, F
De Portu, G
Anglada, M
Llanes, L [1 ]
机构
[1] Univ Politecn Catalunya, ETSEIB, Dept Ciencia Mat & Engn Met, E-08028 Barcelona, Spain
[2] SOFC, Res Ctr Juelich, D-52425 Julich, Germany
[3] Natl Res Council, Res Inst Ceram Technol, I-48018 Faenza, Italy
关键词
PSZ; fatigue; racture; toughness; ZrO2;
D O I
10.1016/S0955-2219(98)00281-7
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The fatigue and fracture characteristics of a partially-stabilized fine-grained zirconia with spinel additions, (Mg, Y)-PSZ, were studied. Fracture toughness, crack growth resistance curves and fatigue crack growth (FCG) behavior, under both sustained and cyclic loading, were evaluated. Mechanical fatigue effects were clearly evidenced by (1) remarkable crack growth rate differences under cyclic and static loading and (2) significant loading Patio effects. Comparing the cyclic and the static FCG behavior allows to deduce a higher cyclic fatigue sensitivity of the fine-grained (Mg, Y)-PSZ with respect to a commercial peak-aged Mg-PSZ used as a reference material. By in situ observation of crack extension under cyclic loading, the fatigue mechanisms could be resolved. Mechanical degradation of bridging ligaments, as already known for coarse-grained Mg-PSZ, is one sour ce of cyclic fatigue. An additional source attributed to the particle dispersed microstructure of the (Mg, Y)-PSZ is the interaction between crack faces and hard spinel particles. The sensitivity of (Mg, Y)-PSZ and Mg-PSZ to cyclic fatigue is discussed in terms of the respective microstructures, prevalence and operativity of distinct mechanical fatigue mechanisms. (C) 1999 Elsevier Science Limited. All rights reserved.
引用
收藏
页码:1705 / 1715
页数:11
相关论文
共 50 条
  • [11] Corrosion behavior of fine grained (Mg,Y)-PSZ ceramics in hot steam environment
    Harbin Univ of Technology, Harbin, China
    Gongneng Cailiao, 6 (653-655):
  • [12] SUPERPLASTIC BULGING OF FINE-GRAINED ZIRCONIA
    XIN, W
    CHEN, IW
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (03) : 746 - 749
  • [14] Preparation and properties of fine-grained (Ce, Mg)-PSZ/MgAl2O4 ceramics
    Ma, Y.L.
    Sun, X.B.
    Zheng, J.P.
    Yuan, Q.M.
    2001, Beijing Institute of Aeronautical Materials (BIAM)
  • [15] Creep behavior of a fine-grained tetragonal zirconia
    Morita, K
    Hiraga, K
    Sakka, Y
    CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 2000, 171-1 : 847 - 854
  • [16] Deformed substructures in fine-grained tetragonal zirconia
    Morita, K
    Hiraga, K
    PHILOSOPHICAL MAGAZINE LETTERS, 2001, 81 (05) : 311 - 319
  • [17] Creep behavior of a fine-grained tetragonal zirconia
    Morita, K.
    Hiraga, K.
    Sakka, Y.
    Key Engineering Materials, 2000, 171-174 : 847 - 854
  • [18] The role of Y2O3 in fine-grained (Y,Mg)PSZ/MgAl2O4 during long term heat treatment
    Zhang, Q
    Chen, YR
    Wu, HZ
    Liu, WX
    Yuan, QM
    CERAMICS INTERNATIONAL, 1998, 24 (03) : 175 - 179
  • [19] Process and properties of fine-grained (Y/Ce,M)-PSZ/MgAl2O4 ceramics
    Ma, YL
    Yuan, QM
    Tan, JQ
    Zhu, XH
    JOURNAL OF INORGANIC MATERIALS, 1998, 13 (04) : 575 - 581
  • [20] Preparation of fine-grained zirconia systems by colloidal processing
    Sakka, Y
    Uchikoshi, T
    Ozawa, K
    Suzuki, TS
    Hiraga, K
    CERAMIC PROCESSING SCIENCE, 1998, 83 : 233 - 240