Methane decomposition and catalyst regeneration in a cyclic mode over supported Co and Ni catalysts
被引:31
作者:
Li, Jerry
[1
]
Smith, Kevin J.
[1
]
机构:
[1] Univ British Columbia, Dept Chem & Biol Engn, Vancouver, BC V6T 1Z3, Canada
基金:
加拿大自然科学与工程研究理事会;
关键词:
Methane decomposition;
Partial oxidation;
Carbon;
Catalyst;
Cobalt;
Nickel;
Cyclic reaction;
D O I:
10.1016/j.apcata.2008.07.011
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
CH4 decomposition (CH4 -> C + 2H(2)) on supported Co and Ni catalysts has been studied using a fixed-bed, oscillating microbalance reactor and a 5% CH4 in He feed reacted at 773 K and 101 kPa. After 45 min reaction the catalysts were regenerated by reaction of the deposited carbon with O-2 or CO2 at 773 K and 101 kPa. The effect of repeated CH4 decomposition-carbon oxidation cycles is reported. At the chosen conditions, Ni was more active and more stable than Co during the CH4 decomposition step. Although > 90% of the carbon deposited on both Co and Ni was removed by reaction with O-2, an oxidation of the active metal also occurred. In subsequent CH4 decomposition steps, an induction period was necessary to re-reduce the Co. Furthermore, the oxidized metal reacted with CH4 producing CO and CO2 as an impurity Removal of the carbon deposit by reaction with CO2 rather than O-2 significantly decreased the in the H-2. CO contamination of the produced H-2 on the Ni catalyst, However, the carbon removal rate was 20x's slower with CO2 compared to O-2. Several CH4 decomposition-carbon oxidation cycles were completed on the Ni catalyst without a significant loss in activity, whereas the Co catalyst deactivated. (c) 2008 Elsevier B.V. All rights reserved.