Investigation on TIG welding of SiCp-reinforced aluminum-matrix composite using mixed shielding gas and Al-Si filler

被引:54
作者
Wang Xi-he [1 ]
Niu Ji-tai [1 ]
Guan Shao-kang [1 ]
Wang Le-jun [1 ]
Cheng Dong-feng [1 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Zhengzhou 450002, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2009年 / 499卷 / 1-2期
关键词
He-Ar mixed gas; SiCp reinforcement; Al matrix composite; TIG welding; MICROSTRUCTURE;
D O I
10.1016/j.msea.2008.07.037
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Using He-Ar mixed gas as shielding gas, the tungsten inert gas (TIG) welding of SiCp/6061 Al composites was investigated without and with Al-Si filler. Welded joint with filler were submitted to tensile tests. The microstructure and fracture morphology of the joint were examined. The results show that adding 50 vol.% helium in shielding gas improves the arc stability, and seams with high-quality appearance are obtained when the AI-Si filler is added. In addition, the interface reaction between SiC and matrix is greatly suppressed when using AI-Si filler. The microstructure of the welded joint displays non-uniformity with many SiC particles distributing in the weld center. The average tensile strength of weld joints with Al-Si filler is 70% above that of the matrix composites under annealed condition. (C) 2008 Elsevier B.V. All rights reserved.