Enhanced diamond nucleation on copper substrates by employing an electrostatic self-assembly seeding process with modified nanodiamond particles

被引:25
作者
Liu, Xuezhang [1 ]
Yu, Tao [1 ]
Wei, Qiuping [1 ,2 ]
Yu, Zhiming [1 ,2 ]
Xu, Xiangyang [3 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
[3] Changsha Res Inst Min & Met, R&D, Changsha 410083, Hunan, Peoples R China
关键词
Nanodiamond seeding; Surface modification; CVD diamond film; Electrostatic self-assembly; Interaction energy; Copper substrate; ELECTRICAL DOUBLE-LAYER; CHEMICAL-VAPOR-DEPOSITION; FORCES; GROWTH; DISPERSION; SURFACES; ADHESION; SILICA; MICA; CVD;
D O I
10.1016/j.colsurfa.2012.07.020
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nanodiamond seeding is a well-established approach to enhancing the nucleation density in chemical vapor deposition (CVD) diamond growth. However, the effects of nanodiamond seeding are highly dependent upon the dispersion properties of nanodiamond particles, the solvent and the interaction between nanoparticles and substrate surfaces. Surface modification and fractionalization were employed to improve the dispersion of nanodiamond particles and separate those particles into a more narrow range of particle size. Mono-dispersed nanodiamonds with a zeta-potential and average particle size of -41.5 mV and similar to 25.3 nm, respectively, were then obtained. They can be charged on copper substrate without any contaminations. Two-dimensional self-assemblies of nanodiamond seeding were actualized. The density and homogeneity of nanodiamond particles which act as pre-existing sp(3) seeds shorten the incubation time of diamond nucleation to less than 30 min. High quality of 750 nm thick continuous diamond film was deposited on copper substrate in 60 min. Furthermore, we calculated electrostatic interaction energy between nanodiamond particle and copper substrate by using the nonlinear Poisson-Boltzmann theory, and discussed interaction energy of nanodiamond-Cu substrate and nanodiamond-nanodiamond in the seeding process. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:82 / 89
页数:8
相关论文
共 43 条
[1]   Chromium interlayers as a tool for enhancing diamond adhesion on copper [J].
Ali, N ;
Ahmed, W ;
Rego, CA ;
Fan, QH .
DIAMOND AND RELATED MATERIALS, 2000, 9 (08) :1464-1470
[2]   Combined substrate polishing and biasing during hot-filament chemical vapor deposition of diamond on copper [J].
Ali, N ;
Ahmed, W ;
Rego, CA ;
Fan, QH .
JOURNAL OF MATERIALS RESEARCH, 2000, 15 (03) :593-595
[3]  
[Anonymous], ROBOTIC MICRO ASSEMB
[4]   Diamond nanoseeding on silicon:: Stability under H2 MPCVD exposures and early stages of growth [J].
Arnault, J. C. ;
Saada, S. ;
Nesladek, M. ;
Williams, O. A. ;
Haenen, K. ;
Bergonzo, P. ;
Osawa, E. .
DIAMOND AND RELATED MATERIALS, 2008, 17 (7-10) :1143-1149
[5]   CALCULATION OF ELECTRIC DOUBLE-LAYER FORCE BETWEEN UNLIKE SPHERES [J].
BELL, GM ;
PETERSON, GC .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1972, 41 (03) :542-566
[6]   Enhancement of the nucleation of smooth and dense nanocrystalline diamond films by using molybdenum seed layers [J].
Buijnsters, J. G. ;
Vazquez, L. ;
van Dreumel, G. W. G. ;
ter Meulen, J. J. ;
van Enckevort, W. J. P. ;
Celis, J. P. .
JOURNAL OF APPLIED PHYSICS, 2010, 108 (10)
[7]   The CVD of nanodiamond materials [J].
Butler, James E. ;
Sumant, Anirudha V. .
CHEMICAL VAPOR DEPOSITION, 2008, 14 (7-8) :145-160
[8]   Electrical double layer interactions between dissimilar oxide surfaces with charge regulation and Stern-Grahame layers [J].
Chan, DYC ;
Healy, TW ;
Supasiti, T ;
Usui, S .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2006, 296 (01) :150-158
[9]   Surface roughness and surface force measurement: A comparison of electrostatic potentials derived from atomic force microscopy and electrophoretic mobility measurements [J].
Considine, RF ;
Drummond, CJ .
LANGMUIR, 2001, 17 (25) :7777-7783
[10]   HFCVD diamond growth on Cu(111). Evidence for carbon phase transformations by in situ AES and XPS [J].
Constant, L ;
Speisser, C ;
LeNormand, F .
SURFACE SCIENCE, 1997, 387 (1-3) :28-43