Orientation relationship between TiB precipitate and γ-TiAl phase

被引:27
作者
Chen, C. L.
Lu, W.
Lin, J. P.
He, L. L.
Chen, G. L.
Ye, H. Q.
机构
[1] Chinese Acad Sci, Met Res Inst, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Beijing 100039, Peoples R China
[3] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
TiAl; interface; orientation relationship; transmission electron microscopy;
D O I
10.1016/j.scriptamat.2006.12.005
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The orientation relationship (OR) and the interface structure between TiB precipitate and gamma-TiAl phase have been investigated using high-resolution electron microscopy. The OR was determined to be [0 (1) over bar0](TiB)parallel to[1 (1) over bar0](gamma), (100)(TiB)parallel to(11 (2) over bar)gamma: This OR has been predicted precisely by the method of coincidence of reciprocal lattice points. The basic vector transformation matrix was also calculated. Based on the investigation of the interface structure, the morphology of the TiB precipitate was discussed from the viewpoint of interface energy. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:441 / 444
页数:4
相关论文
共 26 条
[1]   Work hardening and recovery of gamma base titanium aluminides [J].
Appel, F ;
Sparka, U ;
Wagner, R .
INTERMETALLICS, 1999, 7 (3-4) :325-334
[2]   Microstructure and deformation of two-phase γ-titanium aluminides [J].
Appel, F ;
Wagner, R .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 1998, 22 (05) :187-268
[3]   Mechanical properties of nanocrystalline Ti-Al-X alloys [J].
Calderon, HA ;
Garibay-Febles, V ;
Umemoto, M ;
Yamaguchi, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 329 :196-205
[4]   The mechanism of grain refinement in TiAl alloys by boron addition - an alternative hypothesis [J].
Cheng, TT .
INTERMETALLICS, 2000, 8 (01) :29-37
[5]  
Christodoulou L, 1996, INT WORKSH GAMM ALL
[6]   THE STRUCTURE OF COMPLEX MONOBORIDES IN GAMMA-TIAL ALLOYS WITH TA AND B-ADDITIONS [J].
DEGRAEF, M ;
LOFVANDER, JPA ;
LEVI, CG .
ACTA METALLURGICA ET MATERIALIA, 1991, 39 (10) :2381-2391
[7]   Effect of boron addition on tensile ductility in lamellar TiAl alloys [J].
Hu, D .
INTERMETALLICS, 2002, 10 (09) :851-858
[8]   Effect of composition on grain refinement in TiAl-based alloys [J].
Hu, D .
INTERMETALLICS, 2001, 9 (12) :1037-1043
[9]   THE EFFECTS OF CR ADDITIONS TO BINARY TIAL-BASE ALLOYS [J].
HUANG, SC ;
HALL, EL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11) :2619-2627
[10]   EVOLUTION OF BORIDE MORPHOLOGIES IN TIAL-B ALLOYS [J].
HYMAN, ME ;
MCCULLOUGH, C ;
LEVI, CG ;
MEHRABIAN, R .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (07) :1647-1662