Failure analysis of Ti6Al4V gas turbine compressor blades

被引:77
作者
Kermanpur, A. [1 ]
Amin, H. Sepehri [1 ]
Ziaei-Rad, S. [2 ]
Nourbakhshnia, N. [2 ]
Mosaddeghfar, M. [3 ]
机构
[1] Isfahan Univ Technol, Dept Mat Engn, Esfahan 8415683111, Iran
[2] Isfahan Univ Technol, Dept Mech Engn, Esfahan 8415683111, Iran
[3] Isfahan Reg Elect Co, Esfahan, Iran
关键词
failure analysis; compressor blades; fretting; fractography; finite element analysis;
D O I
10.1016/j.engfailanal.2007.11.018
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The failure mechanism of Ti6A14V compressor blades of an industrial gas turbine was analysed by means of both experimental characterisations and numerical simulation techniques. Several premature failures were occurred in the high pressure section of the compressor due to the fracture of the blade roots. Metallurgical and mechanical properties of the blade alloy were evaluated. A 2D finite element model of the blade root was constructed and used to provide accurate estimates of stress field in the dovetail blade root and to determine the crack initiation in the dovetail. The results showed no metallurgical and mechanical deviations for the blade materials from standards. SEM fractography showed different aspects of fretting fatigue including multiple crack initiation sites, fatigue beach marks, debris particles, and a high surface roughness in the edge of contact (EOC). The numerical model clearly showed the region of highest stress concentration at the front EOC of the blade root in the dovetail region, correlated closely with the experimentally characterised fatigue crack region. It was concluded that this failure has occurred due to the tight contact between the blade root and the disk in the dovetail region as well as low wear resistance of the blade root. (C) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1052 / 1064
页数:13
相关论文
共 17 条
  • [1] *AMS, 2001, 4928Q AMS SAE INT
  • [2] [Anonymous], 1991, ADV SURFACE COATINGS
  • [3] Arrieta HV, 2003, RTOMPAVT109
  • [4] BURNS C, 2002, P 7 NAT TURB ENG HIG
  • [5] A fracture mechanics life prediction methodology applied to dovetail fretting
    Golden, P. J.
    Calcaterra, J. R.
    [J]. TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1172 - 1180
  • [6] Effect of high temperature on the characterization of fretting wear regimes at Ti6Al4V interfaces
    Hager, CH
    Sanders, JH
    Sharma, S
    [J]. WEAR, 2006, 260 (4-5) : 493 - 508
  • [7] The analysis and prevention of failure in railway axles
    Hirakawa, K
    Toyama, K
    Kubota, M
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 1998, 20 (02) : 135 - 144
  • [8] Effect of various surface conditions on fretting fatigue behavior of Ti-6Al-4V
    Hutson, AL
    Niinomi, M
    Nicholas, T
    Eylon, D
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (12) : 1223 - 1234
  • [9] Progression of fretting fatigue damage in Ti-6Al-4V
    Hutson, Alisha
    Sathish, Shamachary
    Nicholas, Ted
    [J]. TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1197 - 1205
  • [10] Effect of dissimilar metals on fretting fatigue behavior of Ti-6Al-4V
    Hutson, Alisha
    Lee, Hyukjae
    Mall, Shankar
    [J]. TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1187 - 1196