Flame retardancy and thermal decomposition of flexible polyurethane foams: Structural influence of organophosphorus compounds

被引:122
作者
Liang, Shuyu [1 ]
Neisius, Matthias [1 ]
Mispreuve, Henri
Naescher, Reinold
Gaan, Sabyasachi [1 ]
机构
[1] Empa Swiss Fed Labs Mat Sci & Technol, Chem Grp, CH-9014 St Gallen, Switzerland
关键词
Foam; Flame retardant; Phosphate; Phosphonate; Phosphoramidate; PO; FIRE-RETARDANCY; PHOSPHORUS-NITROGEN; COMBUSTION; PHOSPHATE; TOXICITY; BEHAVIOR; ACID;
D O I
10.1016/j.polymdegradstab.2012.07.019
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this study the structural effect of different phosphorus compounds on the flame retardant (FR) properties of flexible polyurethane foams (FPUF) was investigated. A series of organophosphorus compounds (phosphonates, phosphates and phosphoramidates) with systematical structure variations were synthesized and incorporated into the flexible foam during its polymerization process. The flame-retarding efficiency of these phosphorus compounds was subsequently evaluated by subjecting their corresponding flame-retarded foams to standard fire tests such as limiting oxygen index (LOI), BKZ-vertical burning test and UL 94-horizontal burning test for foamed materials. It was observed that the synthesized phosphonates and analogous phosphoramidates were more effective than the corresponding phosphates. The presence of an allyl moiety within the molecular structure further improved the FR efficacy of the phosphonate and phosphoramidate compounds, whereas a benzyl group reduced the flame retardant efficiency significantly. The thermogravimetric (TGA) analysis and pyrolysis combustion flow calorimetry (PCFC) results for the FPUF indicated that the most effective FRs might act predominantly in gas phase and exhibit lower condensed phase action (i.e. catalyze the decomposition of FPUF to happen at lower temperatures). Mass spectrometric analysis of FRs indicates that phosphonate and phosphoramidate derivatives appear to support the phosphoryl radical formation more than the investigated phosphate compounds. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2428 / 2440
页数:13
相关论文
共 43 条
[1]  
[Anonymous], 1991, National school district partnership survey. Statistical report, P1
[2]  
BABUSHOK V, 1999, P 3 INT C FIR RES EN, P257
[3]  
Balbo B, 2011, US patent application publication, Patent No. 0190407
[4]  
Bayer AG, 2003, ADDITIVES POLYM, V2003, P3
[5]  
Benbow AW, COMBUSTION FLAME, V24, P217
[6]   THE THERMAL-DECOMPOSITION OF POLYURETHANES AND POLYISOCYANURATES [J].
CHAMBERS, J ;
JIRICNY, J ;
REESE, CB .
FIRE AND MATERIALS, 1981, 5 (04) :133-141
[7]   Transition from smoldering to flaming combustion of horizontally oriented flexible polyurethane foam with natural convection [J].
Chao, CYH ;
Wang, JH .
COMBUSTION AND FLAME, 2001, 127 (04) :2252-2264
[8]   Thermal stability and flame retardancy of polyurethanes [J].
Chattopadhyay, D. K. ;
Webster, Dean C. .
PROGRESS IN POLYMER SCIENCE, 2009, 34 (10) :1068-1133
[9]  
Duquesne S, 2001, J APPL POLYM SCI, V82, P3262, DOI 10.1002/app.2185
[10]   Chronic toxicity and carcinogenic potential of tris-(1,3-dichloro-2-propyl) phosphate in Sprague-Dawley rat [J].
Freudenthal, RI ;
Henrich, RT .
INTERNATIONAL JOURNAL OF TOXICOLOGY, 2000, 19 (02) :119-125