New Failure Mode of Flip-Chip Solder Joints Related to the Metallization of an Organic Substrate

被引:1
作者
Jang, J. W. [1 ]
Yoo, S. J. [1 ]
Hwang, H. I. [1 ]
Yuk, S. Y. [1 ]
Kim, C. K. [1 ]
Kim, S. J. [1 ]
Han, J. S. [1 ]
An, S. H. [1 ]
机构
[1] Samsung Elect, Test & Package Ctr, Chungnam 336711, South Korea
关键词
Flip chip; OSP; Cl ion; corrosion; thermomechanical stress; CRACKING;
D O I
10.1007/s11664-015-3817-2
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
We report a new failure phenomenon during flip-chip die attach. After reflow, flip-chip bumps were separated between the Al and Ti layers on the Si die side. This was mainly observed at the Si die corner. Transmission electron microscopy images revealed corrosion of the Al layer at the edge of the solder bump metallization. The corrosion at the metallization edge exhibited a notch shape with high stress concentration factor. The organic substrate had Cu metallization with an organic solderable preservative (OSP) coating layer, where a small amount of Cl ions were detected. A solder bump separation mechanism is suggested based on the reaction between Al and Cl, related to the flow of soldering flux. During reflow, the flux will dissolve the Cl-containing OSP layer and flow up to the Al layer on the Si die side. Then, the Cl-dissolved flux will actively react with Al, forming AlCl3. During cooling, solder bumps at the Si die corner will separate through the location of Al corrosion. This demonstrated that the chemistry of the substrate metallization can affect the thermomechanical reliability of flip-chip solder joints.
引用
收藏
页码:3957 / 3961
页数:5
相关论文
共 16 条
  • [1] Banijamali B., 2009, 59 EL COMP TECHN C S, P293
  • [2] Barin I., 1989, THERMOCHEMICAL DAT 1, P31
  • [3] Gilleo K., 2002, ARRAY PACKAGING HDB
  • [4] Holden H., 2013, THE PCB MAGAZINE JUN, P12
  • [5] High-lead flip chip bump cracking on the thin organic substrate in a module package
    Jang, J. W.
    Li, L.
    Bowles, P.
    Bonda, R.
    Frear, D. R.
    [J]. MICROELECTRONICS RELIABILITY, 2012, 52 (02) : 455 - 460
  • [6] Interfacial morphology and shear deformation of flip chip solder joints
    Jang, JW
    Liu, CY
    Kim, PG
    Tu, KN
    Mal, AK
    Frear, DR
    [J]. JOURNAL OF MATERIALS RESEARCH, 2000, 15 (08) : 1679 - 1687
  • [7] Joshi M., 2010, 60 EL COMP TECHN C L, P1250
  • [8] Joy D.C., 1986, PRINCIPLES ANAL ELEC, pChap 4
  • [9] Lee H.-S., 2007, J MICROELECTRONICS P, V14, P1
  • [10] Flip-Chip-Assembled W-Band CMOS Chip Modules on Ceramic Integrated Passive Device With Transition Compensation for Millimeter-Wave System-in-Package Integration
    Lu, Hsin-Chia
    Kuo, Che-Chung
    Lin, Po-An
    Tai, Chen-Fang
    Chang, Yi-Long
    Jiang, Yu-Sian
    Tsai, Jeng-Han
    Hsin, Yue-Ming
    Wang, Huei
    [J]. IEEE TRANSACTIONS ON MICROWAVE THEORY AND TECHNIQUES, 2012, 60 (03) : 766 - 777