Study on microstructure and electrochemical performance of La0.7Mg0.3(Ni0.9Co0.1)x hydrogen storage alloys

被引:21
作者
Cheng, L. F. [1 ]
Wang, R. B. [2 ]
Pu, Z. H. [2 ]
Li, Z. L. [2 ]
He, D. N. [1 ]
Xia, B. J. [2 ]
机构
[1] Natl Engn & Res Ctr Nanotechnol, Shanghai 200241, Peoples R China
[2] Chinese Acad Sci, Shanghai Inst Microsyst & Informat Technol, Shanghai 200050, Peoples R China
关键词
Hydrogen storage alloy; La2Ni7; phase; Electrochemical properties;
D O I
10.1016/j.jpowsour.2008.08.005
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Hydrogen storage alloys La-0.7 Mg-0.3(Ni-0.9)Co-0.1)(x) (x = 3.0, 3.1, 3.3, 3.4, 3.5, 3.7 and 3.8) were prepared by inductive melting followed by annealing treatment at 1173 K for 6 h. The effects of the stoichiometry (x) on the structural and electrochemical characteristics of the alloys were investigated systematically. Xray diffraction (XRD). optical morphology and energy dispersive spectrometry (EDS) analyses showed that these alloys have a multiphase structure which consists of a (La, Mg)Ni-3 phase with the PuNi3-type rhombohedral structure, a LaNi5 phase with the CaCu5-type hexagonal structure and a (La, Mg)(2)Ni-7 phase with the Ce2Ni7-type hexagonal structure. The main phase of the alloys with x = 3.0 and 3.1 is (La, Mg)Ni-3 phase (PuNi3-type Structure), the main phase of the alloys with x = 3.3, 3.4 and 3.5 is (La, Mg)(2)Ni-7 phase (Ce2Ni7-type structure), and the main phase of the alloys with x = 3.7 and 3.8 is LaNi5 phase (CaCu5-type structure). Moreover, the lattice parameters of the (La, Mg)Ni-3 phase, (La, Mg)(2)Ni-7 phase and LaNi5 phase decrease monotonously with the increase of the value x. The electrochemical analysis shows that the maximum discharge capacity increases from 356.6 mA hg(-1) (x=3.0) to 392.1 mAh g(-1) (x=3.5) and then decreases to 344.1 mA hg(-1) (x=3.8), and the alloys exhibit good cycling stability. As the discharge Current density is 3000 mAg(-1). the high-rate dischargeability (HRD) increases from 30.1 % (x= 3.0) to 56.1 % (x=3.8). The low temperature dischargeability (LTD) increases from 24.3%(x=3.0) to 58.96% (x=3.7) and then decreases to 48.1 % (x = 3.8). (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:1519 / 1523
页数:5
相关论文
共 50 条
[21]   Crystallographic and Electrochemical Hydrogen Storage Characteristics of La0.7Ce0.3Ni4.2Mn0.9-xCu0.3(W0.42Fe0.58)x alloys [J].
Ma, Mingjie ;
Shi, Jianchao ;
He, Chen ;
Fan, Yanping ;
Zhang, Baoqi Ng ;
Sun, Junling .
INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2015, 10 (09) :7631-7642
[22]   Crystallographic and electrochemical characteristics of La0.7Mg0.3Ni3-x(Al0.5Mo0.5)x (x=0-0.4) hydrogen storage alloys [J].
Zhang, XB ;
Sun, DZ ;
Yin, WY ;
Chai, YJ ;
Zhao, MS .
ELECTROCHIMICA ACTA, 2005, 50 (16-17) :3407-3413
[23]   Microstructure and electrochemical properties of La0.8-xMMxMg0.2Ni3.1Co0.3Al0.1 (x=0, 0.1, 0.2, 0.3) alloys [J].
Zhou, Na ;
Du, Wen-Bo ;
Zhang, Pei-Long ;
Zhu, Yong-Guo ;
Wang, Zhao-Hui ;
Liu, Ke ;
Li, Shu-Bo .
RARE METALS, 2017, 36 (08) :645-650
[24]   Structure and electrochemical properties of La0.7Mg0.3Ni2.45-xCo0.75Mn0.1Al0.2Wx (x=0-0.15) hydrogen storage alloys [J].
Pan, HG ;
Wu, XF ;
Gao, MX ;
Chen, N ;
Yue, YJ ;
Lei, YQ .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (04) :517-523
[25]   The effect of Mn substitution for Ni on the structural and electrochemical properties of La0.7Mg0.3Ni2.55-xCo0.45Mnx hydrogen storage electrode alloys [J].
Liu, YF ;
Pan, HG ;
Gao, MX ;
Zhu, YF ;
Lei, YQ ;
Wang, QD .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2004, 29 (03) :297-305
[26]   The effect of substitution of Zr for La on the electrochemical properties of La0.7-xZrxMg0.3Ni2.45Mn0.1Co0.75Al0.2 hydrogen storage electrode alloys [J].
Pan, HG ;
Yue, YJ ;
Gao, MX ;
Wu, XF ;
Chen, N ;
Lei, YQ ;
Wang, QD .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 397 (1-2) :269-275
[27]   Microstructure and electrochemical properties of La0.8–xMMxMg0.2Ni3.1Co0.3Al0.1 (x = 0, 0.1, 0.2, 0.3) alloys [J].
Na Zhou ;
Wen-Bo Du ;
Pei-Long Zhang ;
Yong-Guo Zhu ;
Zhao-Hui Wang ;
Ke Liu ;
Shu-Bo Li .
Rare Metals, 2017, 36 :645-650
[28]   Microstructure and electrochemical performances of La0.7Mg0.3Ni2.55-xCo0.45Cux (x=0-0.4) hydrogen storage alloys prepared by casting and rapid quenching [J].
Zhang, Yang-Huan ;
Dong, Xiao-Ping ;
Wang, Guo-Qing ;
Guo, Shi-Hai ;
Ren, Jiang-Yuan ;
Wang, Xin-Lin .
JOURNAL OF ALLOYS AND COMPOUNDS, 2006, 417 (1-2) :224-229
[29]   Effects of heat treatment on electrochemical properties of La0.7Mg0.3Ni2.8Co0.5 hydrogen storage alloy [J].
Liu, YF ;
Jin, QW ;
Gao, MX ;
Zhu, YF ;
Zhang, ZH ;
Pan, HG .
RARE METAL MATERIALS AND ENGINEERING, 2003, 32 (11) :942-945
[30]   Influences of Co substitution and annealing treatment on the structure and electrochemical properties of hydrogen storage alloys La0.7Mg0.3Ni2.45-xCo0.75+xMn0.1Al0.2 (x=0.00, 0.15, 0.30) [J].
Miao, He ;
Pan, Hongge ;
Zhang, Shengcai ;
Chen, Ni ;
Li, Rui ;
Gao, Mingxia .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (15) :3387-3394