Control of magnetite primary particle size in aqueous dispersions of nanoclusters for high magnetic susceptibilities

被引:17
|
作者
Yoon, Ki Youl [1 ]
Xue, Zheng [1 ]
Fei, Yunping [1 ]
Lee, Jae Ho [1 ]
Cheng, Victoria [1 ]
Bagaria, Hitesh G. [1 ]
Huh, Chun [2 ]
Bryant, Steven L. [2 ]
Kong, Seong Deok [1 ]
Ngo, Vincent W. [1 ]
Rahmani, Amir-Reza [2 ]
Ahmadian, Mohsen [3 ,4 ]
Ellison, Christopher J. [1 ]
Johnston, Keith P. [1 ]
机构
[1] Univ Texas Austin, Dept Chem Engn, Austin, TX 78712 USA
[2] Univ Texas Austin, Dept Petr & Geosyst Engn, Austin, TX 78712 USA
[3] Univ Texas Austin, Adv Energy Consortium, Austin, TX 78758 USA
[4] Univ Texas Austin, Bur Econ Geol, Austin, TX 78758 USA
关键词
Superparamagnetic nanoparticles; Magnetite Electromagnetic imaging; Magnetic susceptibility; Aqueous dispersion; Colloidal stability; IRON-OXIDE NANOPARTICLES; SULFONATED COPOLYMERS; FREQUENCY-DEPENDENCE; CONCENTRATED BRINE; STABILITY; FUNCTIONALIZATION; NANOCRYSTALS; SEPARATION; SILICA; FLUIDS;
D O I
10.1016/j.jcis.2015.09.058
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Aqueous dispersions of iron oxide nanoparticles with a high initial magnetic susceptibility (xi) are of interest as contrast agents in electromagnetic tomography. Nanoclusters composed of iron oxide primary particles were formed by co-precipitation of Fe(II) and Fe(III) chlorides at alkaline conditions and high temperature of 95 degrees C. Two-step addition of citrate was used to produce large primary particles and then stabilize the nanoclusters. The size of the primary particles was tuned from 5 nm to 15 nm by varying the citrate/iron precursor ratio during the normal phase hydrolysis reaction, while the second iteration of citrate stabilized the nanoclusters with hydrodynamic diameters of 30-75 nm. The crystallinity of the iron oxide nanoparticles was promoted by annealing at 95 degrees C and systematically studied with Superconducting Quantum Interference Device (SQUID), Vibrating Sample Magnetometer (VSM), Transmission Electron Microscopy (TEM) and X-ray Diffraction (XRD). The dependence of xi was examined over a range of low volume fractions (0.005 < 0 < 0.02) to understand the magnetic behavior of dispersions. The xi of the dispersions increased markedly with the size and concentration of the constituent primary particles, reaching an unusually high value of 0.85 at 1.6% v/v for 15 nm primary particles, which is 2-3 times higher than that for typical commercial ferrofluids. The high chi(i) values are favored by the high crystallinity and the large magnetic diameter of 9.3 nm, indicating a relatively thin surface nonmagnetic layer where the spin orientations are disordered. (C) 2015 Published by Elsevier Inc.
引用
收藏
页码:359 / 367
页数:9
相关论文
共 50 条
  • [1] Aqueous Superparamagnetic Magnetite Dispersions with Ultrahigh Initial Magnetic Susceptibilities
    Fei, Yunping
    Iqbal, Muhammad
    Kong, Seong D.
    Xue, Zhen
    McFadden, Charles P.
    Guillet, Jesse L.
    Doerrer, Linda H.
    Alp, Esen E.
    Bi, Wenli
    Lu, Yi
    Dandamudi, Chola B.
    Ranganath, Prashant J.
    Javier, Kevin J.
    Ahmadian, Mohsen
    Ellison, Christopher J.
    Johnston, Keith P.
    LANGMUIR, 2018, 34 (02) : 622 - 629
  • [2] PARTICLE SIZE IN AQUEOUS STARCH DISPERSIONS
    BABCOCK, GE
    TOBIN, R
    DIMLER, RJ
    SENTI, FR
    CEREAL CHEMISTRY, 1960, 37 (05) : 645 - 655
  • [3] Synthesis, Morphology, and Particle Size Control of Acidic Aqueous Polyurethane Dispersions
    Quane, Ellen J.
    Elders, Niels
    Newman, Anna S.
    van Mourik, Sophia
    Williams, Neal S. J.
    van den Berg, Keimpe J.
    Ryan, Anthony J.
    Mykhaylyk, Oleksandr O.
    MACROMOLECULES, 2024, 57 (22) : 10623 - 10634
  • [4] PARTITIONING AND STABILITY OF AQUEOUS DISPERSIONS - PARTICLE-SIZE OF DYE DISPERSIONS
    KISSA, E
    LANGMUIR, 1990, 6 (02) : 478 - 481
  • [5] Interactions at the CMC/magnetite interface: Implications for the stability of aqueous dispersions and the magnetic properties of magnetite nanoparticles
    Maccarini, M.
    Atrei, A.
    Innocenti, C.
    Barbucci, R.
    COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2014, 462 : 107 - 114
  • [6] Preparation of Ethylcellulose Latex by Aqueous Dispersions: Importance of the Particle Size and Plasticizer
    Iqbal, Mahmood
    Chuai, Chengzhi
    Mahmood, Kalsoom
    Huang, Yan
    Liu, Hui
    Aijaz, Muhammad
    JOURNAL OF THE CHEMICAL SOCIETY OF PAKISTAN, 2011, 33 (05): : 634 - 639
  • [7] SIZE-OPTIMIZED MAGNETITE NANOPARTICLES FOR MAGNETIC PARTICLE IMAGING
    Ferguson, R. Matthew
    Khandhar, Amit P.
    Minard, Kevin R.
    Krishnan, Kannan M.
    MAGNETIC NANOPARTICLES: PARTICLE SCIENCE, IMAGING TECHNOLOGY, AND CLINICAL APPLICATIONS, 2010, : 53 - +
  • [8] Magnetic Hysteresis Properties of Magnetite: Trends With Particle Size and Shape
    Paterson, Greig A.
    Moreno, Roberto
    Muxworthy, Adrian R.
    Nagy, Lesleis
    Williams, Wyn
    Tauxe, Lisa
    GEOCHEMISTRY GEOPHYSICS GEOSYSTEMS, 2024, 25 (08)
  • [9] Synthesis, Morphology, and Particle Size Control of Acidic Aqueous Polyurethane Dispersions (vol 57, pg 10623, 2024)
    Quane, Ellen J.
    Elders, Niels
    Newman, Anna S.
    van Mourik, Sophia
    Williams, Neal S. J.
    van den Berg, Keimpe J.
    Ryan, Anthony J.
    Mykhaylyk, Oleksandr O.
    MACROMOLECULES, 2025, 58 (06) : 3355 - 3355
  • [10] Blends of aqueous polymer dispersions used for pellet coating: Importance of the particle size
    Siepmann, F
    Siepmann, J
    Walther, M
    MacRae, RJ
    Bodmeier, R
    JOURNAL OF CONTROLLED RELEASE, 2005, 105 (03) : 226 - 239