摘要
Beta-spodumene (Li(2)O(.)Al(2)O(3)(.)4SiO(2), LAS) powders were prepared by a sol-gel process using Si(OC2H5)(4), A1(OC4H9)(3), and LiNO3 as precursors and LiF as a sintering aid agent. Dilatometry, X-ray diffraction (XRD), scanning electron microscopy (SEM), scanning transmission electron microscopy (STEM), and electron diffraction (ED) were utilized to study the sintering, phase transformation, microstructure, and properties of the)beta-spodumene glass-ceramics prepared from the gel-derived precursor powders with and without LiF additives. For the LAS precursor powders containing no LiF, the only crystalline phase obtained was beta-spodumene. For the pellets containing less than 4 wt pct LiF and sintered at 1050 degreesC for 5 hours the crystalline phases were beta-spodumene and beta-eucryptite (Li(2)O(.)A1(2)O(3)(.)2SiO(2)). When the LiF content was 5 wt pct and the sintering process was carried out at 1050 degreesC for 5 hours, the crystalline phases were beta-spodumene, beta-eucryptite (triclinic), and eucryptite (rhombohedral (hex.)) phases. With the LiF additive increased from 0.5 to 4 wt pct and sintering at 1050 degreesC for 5 hours, the open porosity of the sintered bodies decrease from 30 to 2.1 pct. The grains size is about to 4 to 5 mum when pellect LAS compact contains LiF 3 wt pct as sintered at 1050 degreesC for 5 hours. The grains size grew to 8 to 25 mum with a remarkable discontinuous grain growth for pellet LAS compact contain LiF 5 wt pct sintered at 1050 degreesC for 5 hours. Relative densities greater than 90 pct could be obtained for the LAS precursor powders with LiF > 2 wt pct when sintered at 1050 degreesC for 5 hours. The coefficient of thermal expansion of the sintered bodies decreased from 8.3 X 10(-7) to 5.2 X 10(-7)degreesC (25 degreesC to 900 degreesC) as the LiF addition increased from 0 to 5 wt pct.
引用
收藏
页码:171 / 181
页数:11
相关论文
共 39 条
  • [31] Preparation and Relaxor Behavior of Barium Strontium Titanate Glass-Ceramics Doped Si-B-O Sintered from Sol-Gel Derived Powders
    Wang, Jiangying
    Zhang, Jingji
    FUNCTIONAL AND ELECTRONIC MATERIALS, 2011, 687 : 370 - 374
  • [32] Structural characterization and electrical properties of lead bismuth zirconate titanate (PbBi4ZrxTi4-xO15) ceramics prepared from sol-gel derived powders
    Park, YI
    Miyayama, M
    Kudo, T
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1999, 107 (06) : 527 - 533
  • [33] Structural characterization and electrical properties of lead bismuth zirconate titanate (PbBi4ZrxTi4-xO15) ceramics prepared from sol-gel derived powders
    Park, Yong-Il
    Miyayama, Masaru
    Kudo, Tetsuichi
    Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan, 1999, 107 (1246): : 527 - 533
  • [34] Enhanced "overall" ionic conductivity in Li1+xAlxTi2- x(PO4)3 (0.3 ≤ x ≤ 0.7) ceramics prepared from sol-gel powders by spark plasma sintering
    Martinez-Chaparro, S.
    Kobylianska, S.
    Sobrados, I.
    Jimenez, R.
    Sanz, J.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (10) : 4248 - 4258
  • [35] Low temperature sintering and microwave dielectric properties of Nd[(Zn0.7Co0.3)0.5Ti0.5]O3 ceramics derived from the powders synthesized by ethylenediaminetetraacetic acid precursor route
    Li, Jiamao
    Wang, Hao
    Tan, Jie
    Fan, Chuangang
    CERAMICS INTERNATIONAL, 2019, 45 (18) : 24044 - 24051
  • [36] Ferroelectric and piezoelectric properties of non-stoichiometric Sr1-xBi2+2x/3Ta2O9 ceramics prepared from sol-gel derived powders
    Jain, R
    Gupta, V
    Mansingh, A
    Sreenivas, K
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 112 (01): : 54 - 58
  • [37] Dielectric and piezoelectric properties of non-stoichiometric Sr1-xBi2+2x/3Ta2O9 ceramics prepared from sol-gel derived powders
    Jain, R
    Gupta, V
    Sreenivas, K
    Mansingh, A
    FERROELECTRICS, 2005, 324 : 153 - 156
  • [38] Influence of Li2CO3 and V2O5 combined additions on the sintering and dielectric properties of Ca0.5Sr0.5TiO3 ceramics prepared from powders synthesized by sol-gel method
    Lamrani, Nouara
    Chaouchi, Ahcene
    Bernard, Jerome
    Itaalit, Brahim
    Houivet, David
    Haussonne, Jean Marie
    Aliouat, Mohamed
    PROCESSING AND APPLICATION OF CERAMICS, 2014, 8 (02) : 101 - 108
  • [39] STUDY ON LOW-TEMPERATURE SYNTHESIS OF LI2O-AL2O3-SIO2 CERAMICS FROM METAL ALKOXIDES .2. LOW-TEMPERATURE SINTERING OF FINE PRECURSOR POWDERS IN LI2O-AL2O3-SIO2 SYSTEM
    SUZUKI, H
    TAKAHASHI, J
    SAITO, H
    NIPPON KAGAKU KAISHI, 1991, (10) : 1319 - 1325