A sintering study on the β-spodumene-based glass ceramics prepared from gel-derived precursor powders with LiF additive

被引:8
|
作者
Wang, MC [1 ]
Wu, NC
Yang, S
Wen, SB
机构
[1] Natl Kaohsiung Univ Appl Sci, Dept Mech Engn, Kaohsiung, Taiwan
[2] Natl Cheng Kung Univ, Dept Mat Sci & Engn, Tainan 70101, Taiwan
[3] Natl Cheng Kung Univ, Dept Resources Engn, Tainan 70101, Taiwan
关键词
D O I
10.1007/s11661-002-0016-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Beta-spodumene (Li(2)O(.)Al(2)O(3)(.)4SiO(2), LAS) powders were prepared by a sol-gel process using Si(OC2H5)(4), A1(OC4H9)(3), and LiNO3 as precursors and LiF as a sintering aid agent. Dilatometry, X-ray diffraction (XRD), scanning electron microscopy (SEM), scanning transmission electron microscopy (STEM), and electron diffraction (ED) were utilized to study the sintering, phase transformation, microstructure, and properties of the)beta-spodumene glass-ceramics prepared from the gel-derived precursor powders with and without LiF additives. For the LAS precursor powders containing no LiF, the only crystalline phase obtained was beta-spodumene. For the pellets containing less than 4 wt pct LiF and sintered at 1050 degreesC for 5 hours the crystalline phases were beta-spodumene and beta-eucryptite (Li(2)O(.)A1(2)O(3)(.)2SiO(2)). When the LiF content was 5 wt pct and the sintering process was carried out at 1050 degreesC for 5 hours, the crystalline phases were beta-spodumene, beta-eucryptite (triclinic), and eucryptite (rhombohedral (hex.)) phases. With the LiF additive increased from 0.5 to 4 wt pct and sintering at 1050 degreesC for 5 hours, the open porosity of the sintered bodies decrease from 30 to 2.1 pct. The grains size is about to 4 to 5 mum when pellect LAS compact contains LiF 3 wt pct as sintered at 1050 degreesC for 5 hours. The grains size grew to 8 to 25 mum with a remarkable discontinuous grain growth for pellet LAS compact contain LiF 5 wt pct sintered at 1050 degreesC for 5 hours. Relative densities greater than 90 pct could be obtained for the LAS precursor powders with LiF > 2 wt pct when sintered at 1050 degreesC for 5 hours. The coefficient of thermal expansion of the sintered bodies decreased from 8.3 X 10(-7) to 5.2 X 10(-7)degreesC (25 degreesC to 900 degreesC) as the LiF addition increased from 0 to 5 wt pct.
引用
收藏
页码:171 / 181
页数:11
相关论文
共 39 条
  • [1] A sintering study on the β-spodumene-based glass ceramics prepared from gel-derived precursor powders with LiF additive
    Moo-Chin Wang
    Nan-Chung Wu
    Sheng Yang
    Shaw-Bing Wen
    Metallurgical and Materials Transactions A, 2002, 33 : 171 - 181
  • [2] SINTERING BEHAVIOR OF GEL-DERIVED SILICA POWDERS AND PRECURSOR RESIN
    STARR, TL
    AMERICAN CERAMIC SOCIETY BULLETIN, 1984, 63 (08): : 994 - 994
  • [3] Preparation of β-spodumene-based glass-ceramic powders by polyacrylamide gel process
    Wu, SQ
    Liu, YY
    He, L
    Wang, FP
    MATERIALS LETTERS, 2004, 58 (22-23) : 2772 - 2775
  • [4] Effect of LiF addition on the phase transition of sinterable β-spodumene precursor powders prepared by a sol-gel process
    Moo-Chin Wang
    Nan-Chung Wu
    Sheng Yang
    Shaw-Bing Wen
    Journal of Materials Research, 2002, 17 : 1960 - 1968
  • [5] Effect of LiF addition on the phase transition of sinterable β-spodumene precursor powders prepared by a sol-gel process
    Wang, MC
    Wu, NC
    Yang, S
    Wen, SB
    JOURNAL OF MATERIALS RESEARCH, 2002, 17 (08) : 1960 - 1968
  • [6] Preparation and properties of barium titanate glass-ceramics sintered from sol–gel-derived powders
    KUI Yao
    Liangying Zhang
    Xi Yao
    Weiguang Zhu
    Journal of Materials Science, 1997, 32 : 3659 - 3665
  • [7] Sintering characteristics and crystallization for sol–gel-derived powders for low-dielectric and low-temperature sintering ceramics
    Shaohong Wang
    Heping Zhou
    Journal of Materials Science: Materials in Electronics, 2004, 15 : 55 - 59
  • [8] GEL-DERIVED AMORPHOUS CESIUM-ALUMINOSILICATE POWDERS USEFUL FOR FORMATION OF POLLUCITE GLASS-CERAMICS
    HOGAN, MA
    RISBUD, SH
    JOURNAL OF MATERIALS RESEARCH, 1991, 6 (02) : 217 - 219
  • [9] LiNbO3-based piezoelectric ceramics prepared from sol-gel derived powders
    Nibou, L
    Manier, M
    Mercurio, JP
    ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 1998, 23 (1-2): : 135 - 138
  • [10] Sintering behavior of ZnO: Mn ceramics fabricated from sol-gel derived nanocrystalline powders
    Bahsi, Z. B.
    Buyukaksoy, A.
    Koseoglu, N. C.
    Oral, A. Y.
    Aslan, M. H.
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2009, 100 (05) : 708 - 712