Hot Deformation Behavior and Microstructural Evolution of Mg-Nd-Zn-Zr Magnesium Alloy

被引:1
|
作者
Wu, Wenxiang [1 ]
Jin, Li [1 ]
Dong, Jie [1 ]
Zhang, Zhenyan [1 ]
Ding, Wenjiang [1 ]
机构
[1] Shanghai Jiao Tong Univ, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
来源
关键词
NZ30K alloy; Microstructural evolution; Hot compression deformation; Precipitate; MG-3ND-0.2ZN-0.4ZR WT.PERCENT ALLOY; DYNAMIC RECRYSTALLIZATION;
D O I
10.4028/www.scientific.net/MSF.747-748.320
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The hot deformation behaviors and microstructural evolution of Mg-3.0Nd-0.2Zn-0.4Zr (wt. %, NZ30K) alloy were investigated by means of the isothermal hot compression tests at temperatures of 350-500 degrees C with strain rates of 0.001, 0.01, 0.1 and 1s(-1). The results showed that the flow stress increased to a peak and then decreased which showed a dynamic flow softening. The flow stress behavior was described by the hyperbolic sine constitutive equation with an average activation energy of 193.8 kJ/mol. The average size of dynamically recrystallized grains of hot deformed NZ30K alloy was reduced by increasing the strain rate and/or decreasing the deformation temperature. A large amount of fine particles precipitated in the grains interior and at the grain boundaries when heated to the compression temperatures and soaked for 5min below 450 degrees C. However, the volume fraction of particles decreased significantly when soaked for 5 min at 500 degrees C, and the coarse particles precipitated mainly at the grain boundaries. Hot deformation at the temperature of 500 C around and at the strain rate range of 0.1s(-1) was desirable for NZ30K alloy.
引用
收藏
页码:320 / 326
页数:7
相关论文
共 50 条
  • [31] Hot deformation behavior and hot workability of Mg-Y-Nd-Zr alloy
    Tang, Weineng
    Chen, Rongshi
    Han, Enhou
    Jinshu Xuebao/Acta Metallurgica Sinica, 2006, 42 (10): : 1096 - 1100
  • [32] Hot deformation behavior and hot workability of Mg-Y-Nd-Zr alloy
    Tang Weineng
    Chen Rongshi
    Han Enhou
    ACTA METALLURGICA SINICA, 2006, 42 (10) : 1096 - 1100
  • [33] EFFECTS OF DEGRADABLE MG-ND-ZN-ZR ALLOY ON OSTEOBLASTIC CELL FUNCTION
    Wang, Y.
    Ouyang, Y.
    Peng, X.
    Mao, L.
    Yuan, G.
    Jiang, Y.
    He, Y.
    INTERNATIONAL JOURNAL OF IMMUNOPATHOLOGY AND PHARMACOLOGY, 2012, 25 (03) : 597 - 606
  • [34] Influence of proteins and cells on in vitro corrosion of Mg-Nd-Zn-Zr alloy
    Zhang, Jian
    Kong, Ni
    Shi, Yongjuan
    Niu, Jialin
    Mao, Lin
    Li, Haiyan
    Xiong, Meiping
    Yuan, Guangyin
    CORROSION SCIENCE, 2014, 85 : 477 - 481
  • [36] Hot deformation behavior of extruded Mg-Zn-Y-Zr alloy
    Xia, Xiangsheng
    Chen, Qiang
    Huang, Shuhai
    Lin, Jun
    Hu, Chuankai
    Zhao, Zude
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 644 : 308 - 316
  • [37] Hot Compression Deformation Behavior of Mg-Gd-Nd-Zr Heat-Resistant Magnesium Alloy
    Xin, Yanhui
    Li, Quan-an
    INTERNATIONAL CONFERENCE ON MATERIALS SCIENCES AND NANOMATERIALS, 2017, 230
  • [38] Hot deformation behavior and microstructural evolution of Mg–Zn–Ca–La alloys
    Jiqiang Qi
    Yuzhou Du
    Bailing Jiang
    Mingjie Shen
    Journal of Materials Research, 2018, 33 : 2817 - 2826
  • [39] Forgeability and die-forging forming of direct chill casting Mg-Nd-Zn-Zr magnesium alloy
    Zheng, Xingwei
    Dong, Jie
    Yin, Dongdi
    Liu, Wencai
    Wang, Fenghua
    Jin, Li
    Ding, Wenjiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (16-17): : 3690 - 3694
  • [40] Microstructural evolution of rolled Mg-5Zn-3Nd(-Zr) alloy
    Yang Lin
    Gao Xiao-dan
    Lin Li
    Zou Peng
    Chen Li-jia
    Liu Zheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S498 - S502