High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [41] High-temperature corrosion of heat-resistant chromonickel steel
    Ivanov D.I.
    Kozhukhov A.A.
    Urazova L.F.
    Steel in Translation, 2016, 46 (3) : 192 - 195
  • [42] Temperature dependent ultrasonic properties of aluminium nitride
    Pandey, D. K.
    Yadav, R. R.
    APPLIED ACOUSTICS, 2009, 70 (03) : 412 - 415
  • [43] High-temperature oxidation and corrosion of structural materials in molten chlorides
    Indacochea, JE
    Smith, JL
    Litko, KR
    Karell, EJ
    Raraz, AG
    OXIDATION OF METALS, 2001, 55 (1-2): : 1 - 16
  • [44] High-Temperature Oxidation and Corrosion of Structural Materials in Molten Chlorides
    J. E. Indacochea
    J. L. Smith
    K. R. Litko
    E. J. Karell
    A. G. Rarez
    Oxidation of Metals, 2001, 55 : 1 - 16
  • [45] THE NEED FOR STANDARD TEST METHODOLOGIES FOR HIGH-TEMPERATURE CORROSION - SIMULATING GASEOUS CORROSION PROCESSES
    BAXTER, DJ
    FORDHAM, RJ
    NORTON, JF
    MATERIALS AT HIGH TEMPERATURES, 1993, 11 (1-4) : 70 - 74
  • [46] Formation and transformation of mineral phases in biomass ashes and evaluation of the feedstocks for application in high-temperature processes
    Reinmoller, Markus
    Schreiner, Marcus
    Laabs, Marcel
    Scharm, Christoph
    Yao, Zhitong
    Guhl, Stefan
    Neuroth, Manuela
    Meyer, Bernd
    Graebner, Martin
    RENEWABLE ENERGY, 2023, 210 : 627 - 639
  • [47] Surface Segregation Process and Its Influence on High-Temperature Corrosion of Iron-Based Alloys Containing Aluminium, Vanadium, Titanium and Germanium
    Sobota, Magdalena
    Idczak, Karolina
    Konieczny, Robert
    Idczak, Rafal
    MATERIALS, 2025, 18 (03)
  • [48] Additive manufacturing of high-performance aluminium nitride ceramics using high solid loading and low viscosity slurry
    Lin, Kunji
    Lin, Lifu
    Qi, Yujie
    Lu, Donglin
    Zhang, Wenduo
    Zong, Xiao
    Wu, Shanghua
    VIRTUAL AND PHYSICAL PROTOTYPING, 2024, 19 (01)
  • [49] Investigation on the high-temperature flow behavior of biomass and coal blended ash
    Xu, Jie
    Yu, Guangsuo
    Liu, Xia
    Zhao, Feng
    Chen, Xueli
    Wang, Fuchen
    BIORESOURCE TECHNOLOGY, 2014, 166 : 494 - 499
  • [50] CHANGES OF CHAR PORE STRUCTURE IN HIGH-TEMPERATURE COAL-GASIFICATION
    LIN, SY
    ZHU, ZB
    HIRATO, M
    NINOMIYA, Y
    HORIO, M
    KAGAKU KOGAKU RONBUNSHU, 1993, 19 (02) : 325 - 332