High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [31] Peculiarities of corrosion damage of low alloy chromium on high-temperature salt corrosion
    Rakitskij, A.M.
    Poryadchenko, N.E.
    Panarina, N.I.
    Oryshich, I.V.
    Samelyuk, A.V.
    Fiziko-Khimicheskaya Mekhanika Materialov, 1995, 31 (02): : 103 - 108
  • [32] Towards high-temperature applications of aluminium alloys enabled by additive manufacturing
    Michi, Richard A.
    Plotkowski, Alex
    Shyam, Amit
    Dehoff, Ryan R.
    Babu, Sudarsanam Suresh
    INTERNATIONAL MATERIALS REVIEWS, 2022, 67 (03) : 298 - 345
  • [33] The Phenomena of Secondary Weight Loss in High-Temperature Coal Pyrolysis
    Zeng, Xiongwei
    Zheng, Shu
    Zhou, Huaichun
    ENERGY & FUELS, 2017, 31 (09) : 10178 - 10185
  • [34] The feasibility of a coal gasifier combined with a high-temperature fuel cell
    Kivisaari, T
    Björnbom, P
    Sylwan, C
    Jacquinot, B
    Jansen, D
    de Groot, A
    CHEMICAL ENGINEERING JOURNAL, 2004, 100 (1-3) : 167 - 180
  • [35] Methods for chemical analysis of aluminium nitride powders for fine ceramics
    Funato, M
    BUNSEKI KAGAKU, 1997, 46 (04) : 319 - 325
  • [36] Corrosion in high-temperature and supercritical water and aqueous solutions: a review
    Kritzer, P
    JOURNAL OF SUPERCRITICAL FLUIDS, 2004, 29 (1-2) : 1 - 29
  • [37] Three examples of high-temperature corrosion of metals by molten glasses
    Rapin, C
    Vilasi, M
    Podor, R
    Carton, A
    Gaillard-Allemand, B
    Berthod, P
    Steinmetz, P
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 1125 - 1132
  • [38] RESEARCH OF HIGH-TEMPERATURE CORROSION OF SiC-COATING ON GRAPHITE
    Askerbekov, Saulet K.
    Chikhray, Evgeniy, V
    Ponkratov, Yuriy, V
    Nikitenkov, Nikolay N.
    BULLETIN OF THE TOMSK POLYTECHNIC UNIVERSITY-GEO ASSETS ENGINEERING, 2019, 330 (06): : 98 - 108
  • [39] HIGH-TEMPERATURE CORROSION OF IRON CHROMIUM-ALLOYS BY TELLURIUM
    MAGARA, M
    TSUJI, T
    NAITO, K
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 1991, 28 (08) : 721 - 731
  • [40] High-Temperature Corrosion Behavior of SiBCN Fibers for Aerospace Applications
    Ji, Xiaoyu
    Wang, Shanshan
    Shao, Changwei
    Wang, Hao
    ACS APPLIED MATERIALS & INTERFACES, 2018, 10 (23) : 19712 - 19720