High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [1] Comparison of the high-temperature corrosion of aluminium nitride, alumina, magnesia and zirconia ceramics by coal ashes
    Himpel, Gert
    Herrmann, Mathias
    Hoehn, Soeren
    CERAMICS INTERNATIONAL, 2015, 41 (07) : 8288 - 8298
  • [2] High-temperature corrosion of silicon carbide ceramics by coal ashes
    Herrmann, M.
    Standke, G.
    Hoehn, S.
    Himpel, G.
    Gestrich, T.
    CERAMICS INTERNATIONAL, 2014, 40 (01) : 1471 - 1479
  • [3] Corrosion Resistance of Ceramics and High-temperature Phase Change of Powders on Cubic Silicon Nitride
    Yao Huai
    Zhu Guanglin
    Du Meng
    PHYSICAL AND NUMERICAL SIMULATION OF MATERIAL PROCESSING VI, PTS 1 AND 2, 2012, 704-705 : 853 - 857
  • [4] Aluminium nitride coatings for protection of diamond at high-temperature in air
    McGeoch, SP
    Waddell, EM
    Clark, CC
    Placido, F
    Gou, Z
    Wort, CJH
    Savage, JA
    WINDOW AND DOME TECHNOLOGIES AND MATERIALS VI, 1999, 3705 : 163 - 169
  • [5] High-temperature metal corrosion during the combustion of coal with high salt content
    Shendrik, T. G.
    Dunayevska, N. I.
    Fateiev, A. I.
    MATERIALS SCIENCE, 2025, : 124 - 133
  • [6] High temperature corrosion of silicon nitride composite ceramics in sulfur-oxygen environments
    王昕
    孙康宁
    李静
    于薛刚
    尹衍升
    杨连喜
    Transactions of Nonferrous Metals Society of China, 2003, (02) : 311 - 314
  • [7] High temperature corrosion of silicon nitride composite ceramics in sulfur-oxygen environments
    Wang, X
    Sun, KN
    Li, J
    Yu, XG
    Yin, YS
    Yang, LX
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 (02) : 311 - 314
  • [8] Low-temperature sintering of high-density aluminium nitride ceramics without additives at high pressure
    Li, X. L.
    Ma, H. A.
    Zuo, G. H.
    Liu, W. Q.
    Zheng, Y. J.
    Li, J. G.
    Li, S. S.
    Jia, X.
    SCRIPTA MATERIALIA, 2007, 56 (12) : 1015 - 1018
  • [9] Study of self-propagating high-temperature synthesis of aluminium nitride using a laser monitor
    Li, L.
    Ilyin, A. P.
    Gubarev, F. A.
    Mostovshchikov, A. V.
    Klenovskii, M. S.
    CERAMICS INTERNATIONAL, 2018, 44 (16) : 19800 - 19808
  • [10] Characterization of the melting behavior of high-temperature and low-temperature ashes
    Xu, Jie
    Zhao, Feng
    Guo, Qinghua
    Yu, Guangsuo
    Liu, Xia
    Wang, Fuchen
    FUEL PROCESSING TECHNOLOGY, 2015, 134 : 441 - 448