Oxidative protection of carbon fibers with poly(carborane-siloxane-acetylene)

被引:36
作者
Keller, TM [1 ]
机构
[1] USN, Res Lab, Adv Mat Sect, Div Chem, Washington, DC 20375 USA
关键词
carbon fibers; carbon composites; oxidation; pyrolysis; thermal analysis;
D O I
10.1016/S0008-6223(01)00092-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Linear carborane-siloxane-acetylenic polymers have been synthesized as precursor materials for thermosets and ceramics for composite applications up to 500 and 1500degreesC, respectively, in an oxidizing environment. The novel linear polymers have the advantage of being extremely easy to process and convert into thermosets or ceramics since they are either liquids at room temperature or low melting solids and are soluble in most organic solvents. Carbon fibers coated with poly(carborane-siloxane-acetylene) forms a protective barrier against oxidation at elevated temperatures. The novel polymer when used as a matrix material (ceramic) was found to protect the carbon fibers from oxidative breakdown. Boron appears to be the key to the unique oxidative stability of the composite compositions. Oxidative studies were performed by thermogravimetric analyses. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:225 / 229
页数:5
相关论文
共 16 条
[1]  
Bucca D, 1997, J POLYM SCI POL CHEM, V35, P1033, DOI 10.1002/(SICI)1099-0518(19970430)35:6<1033::AID-POLA6>3.0.CO
[2]  
2-5
[3]  
Bucca D, 1999, J POLYM SCI POL CHEM, V37, P4356, DOI 10.1002/(SICI)1099-0518(19991201)37:23<4356::AID-POLA12>3.0.CO
[4]  
2-3
[5]  
DELMONTE J, 1981, TECHNOLOGY CARBON GR
[6]  
GRAY PE, 1990, Patent No. 4894286
[7]   SYNTHESIS AND CHARACTERIZATION OF POLY(CARBORANE SILOXANE ACETYLENE) [J].
HENDERSON, LJ ;
KELLER, TM .
MACROMOLECULES, 1994, 27 (06) :1660-1661
[8]  
Houser EJ, 1998, J POLYM SCI POL CHEM, V36, P1969, DOI 10.1002/(SICI)1099-0518(199808)36:11<1969::AID-POLA34>3.0.CO
[9]  
2-A
[10]  
Pehrsson PE, 1996, SURF INTERFACE ANAL, V24, P145, DOI 10.1002/(SICI)1096-9918(199603)24:3<145::AID-SIA89>3.0.CO