Fatigue Behavior of Welded T-Joints with a CHS Brace and CFCHS Chord under Axial Loading in the Brace

被引:67
作者
Wang, Ke [1 ,2 ]
Tong, Le-Wei [1 ]
Zhu, Jun [3 ,4 ]
Zhao, Xiao-Ling [5 ,6 ]
Mashiri, Fidelis R. [7 ,8 ]
机构
[1] Tongji Univ, State Key Lab Disaster Reduct Civil Engn, Shanghai 200092, Peoples R China
[2] AECOM Asia Co Ltd, Hong Kong, Hong Kong, Peoples R China
[3] Tongji Univ, State Key Lab Disaster Reduct Civil Engn, Shanghai 200041, Peoples R China
[4] East China Architecture Design & Res Inst, Shanghai, Peoples R China
[5] Monash Univ, Dept Civil Engn, Clayton, Vic 3168, Australia
[6] Tongji Univ, Sch Civil Engn, Shanghai 200092, Peoples R China
[7] Univ Western Sydney, Sch Engn, Penrith, NSW 2751, Australia
[8] Tongji Univ, Sch Civil Engn, Shanghai 20092, Peoples R China
关键词
Welded truss joints; Circular hollow sections; Concrete-filled chords; Hot spot stress; Fatigue tests; Crack initiation and growth; S-N curve; STRESS;
D O I
10.1061/(ASCE)BE.1943-5592.0000331
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The welded truss composed of circular hollow section (CHS) braces and concrete-filled circular hollow-section (CFCHS) chords is a new kind of structural system that has been increasingly applied in large span arch bridges in China. It is necessary to have a good knowledge of fatigue strength of the welded CHS-to-CFCHS joints for the design of this kind of composite bridge. This paper reports on a series of tests on welded CHS-to-CFCHS T-joints subjected to axial cyclic fatigue loading in the brace. Eleven joints were designed to investigate various influence factors such as different nondimensional geometric parameters of circular hollow sections and different concrete strength grades. The quality of welds connecting brace and chord members were examined using the magnetic particle and radiographic inspection methods. The conditions of hot spot stress at both the crown and saddle positions in brace and chord members were determined by means of linear and nonlinear extrapolation methods. During the fatigue testing process, the number of cycles relating to several stages of failure, the crack initiation positions, crack propagation patterns, and the final failure modes were recorded. Fatigue strength of the CHS-to-CFCHS T-joints was compared with that of CHS-to-CHS T-joints. It is concluded that the CHS-to-CFCHS T-joints have a much lower stress concentration factor and consequently have better fatigue strength than the CHS-to-CHS T-joints, when both kinds of joints have the same nondimensional geometrical parameters and same nominal stresses on the brace. The S-rhs-N-f curves in the Comite International pour le Developpement et l'Etude de la Construction Tubulaire guidelines used for CHS-to-CHS joints are not appropriate for the reliable fatigue assessment of CHS-to-CFCHS T-joints based on the current test data. DOI: 10.1061/(ASCE)BE.1943-5592.0000331. (C) 2013 American Society of Civil Engineers.
引用
收藏
页码:142 / 152
页数:11
相关论文
共 27 条
  • [1] ABS, 2004, GUID BUCKL ULT STREN
  • [2] American Welding Society, 2020, AWS D1 1
  • [3] American Welding Society (AWS), 2008, D1108 ANSIAWS
  • [4] API, 2005, REC PRACT PLANN DES
  • [5] Experiment investigation of stress concentration factor of concrete-filled tubular T joints
    Chen, Juan
    Chen, Ju
    Jin, Wei-liang
    [J]. JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2010, 66 (12) : 1510 - 1515
  • [6] de Back J., 1984, 2 INT C WELD TUB STR, P419
  • [7] DNV, 2005, FAT STRENGTH AN OFFS
  • [8] ECCS (European Convention for Constructional Steelwork), 1985, REC FAT DES STEEL ST
  • [9] Efthymiou M., 1998, P OFFSH TUB JOINTS C
  • [10] European Committee for Standardization (CEN), 1992, EUR 3