Effects of SiC interphase by chemical vapor deposition on the properties of C/ZrC composite prepared via precursor infiltration and pyrolysis route

被引:44
作者
Chen, Si'an [1 ]
Zhang, Yudi [1 ]
Zhang, Changrui [1 ]
Zhao, Dan [1 ]
Hu, Haifeng [1 ]
Zhang, Zhibin [2 ]
机构
[1] Natl Univ Def Technol, Sci & Technol Adv Ceram Fibers & Composites Lab, Changsha 410073, Hunan, Peoples R China
[2] China Aerosp Sci & Technol Corp, Inst 4, Xiaogan 432100, Hubei Province, Peoples R China
基金
中国国家自然科学基金;
关键词
Ceramic matrix composites; Silicon carbide; Interphase; Chemical vapor deposition; Carbo-thermal reduction; MECHANICAL-PROPERTIES; SICF/SIC COMPOSITES; FABRICATION; RESISTANCE; ABLATION; BEHAVIOR;
D O I
10.1016/j.matdes.2012.09.019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Silicon carbide (SiC) interphase was introduced by chemical vapor deposition (CVD) process to prevent carbon fiber degradation and improve fiber-matrix interface bonding of C/ZrC composite prepared via precursor infiltration and pyrolysis (PIP) process. Moderate thickness of SiC interphase in fiber bundles could increase the density of the composite, but when the thickness of SiC interphase was over 0.5 mu m, more close pores formed and the density of the composite decreased. The SiC interphase could protect carbon fiber effectively from carbo-thermal reduction, but could not enhance the mechanical properties of C/ZrC composite. The flexural strength and fracture toughness of C/ZrC composites with 0.05 mu m thickness SiC layer were 252 MPa and 13.6 MPa m(1/2), and for those with 0.5 mu m thickness SiC layer 240 MPa and 12.8 MPa m(1/2), both close to the value of the composite without SiC interphase (254 MPa and 14.5 MPa m(1/2)), while those with 0.7 mu m thickness SiC layer were only 191 MPa and 10.8 MPa m(1/2), respectively. Moderate content of SiC interphase could improve the ablation property of C/ZrC composites; however excessive content of SiC interphase would decrease the ablation property. Crown Copyright (C) 2012 Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:497 / 502
页数:6
相关论文
共 26 条
[1]  
Kontinos DA, 20012886 AIAA
[2]   Evaluation of ultra-high temperature ceramics for aeropropulsion use [J].
Levine, SR ;
Opila, EJ ;
Halbig, MC ;
Kiser, JD ;
Singh, M ;
Salem, JA .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (14-15) :2757-2767
[3]   Fabrication of 2D C/ZrC-SiC composite and its structural evolution under high-temperature treatment up to 1800 °C [J].
Li, Houbu ;
Zhang, Litong ;
Cheng, Laifei ;
Wang, Yiguang .
CERAMICS INTERNATIONAL, 2009, 35 (07) :2831-2836
[4]   Boron nitride coatings by chemical vapor deposition from borazine [J].
Li, Jun-Sheng ;
Zhang, Chang-Rui ;
Li, Bin ;
Cao, Feng ;
Wang, Si-Qing .
SURFACE & COATINGS TECHNOLOGY, 2011, 205 (12) :3736-3741
[5]   Fabrication and Properties of 3-D Cf/SiC-ZrC Composites, Using ZrC Precursor and Polycarbosilane [J].
Li, Qinggang ;
Dong, Shaoming ;
Wang, Zhen ;
He, Ping ;
Zhou, Haijun ;
Yang, Jinshan ;
Wu, Bin ;
Hu, Jianbao .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (04) :1216-1219
[6]   Atomic-scale microstructure and elastic properties of quaternary Zr-Al-Si-C ceramics [J].
Lin, Z. J. ;
He, L. F. ;
Wang, J. Y. ;
Li, M. S. ;
Bao, Y. W. ;
Zhou, Y. C. .
ACTA MATERIALIA, 2008, 56 (09) :2022-2031
[7]   Nanoscale twinning-induced elastic strengthening in silicon carbide nanowires [J].
Lin, Z. J. ;
Wang, Lin ;
Zhang, Jianzhong ;
Guo, Xiang-Yun ;
Yang, Wenge ;
Mao, Ho-Kwang ;
Zhao, Yusheng .
SCRIPTA MATERIALIA, 2010, 63 (10) :981-984
[8]   Effects of the single layer CVD SiC interphases on the mechanical properties of the SiCf/SiC composites fabricated by PIP process [J].
Liu, Haitao ;
Cheng, Haifeng ;
Wang, Jun ;
Tang, Gengping .
CERAMICS INTERNATIONAL, 2010, 36 (07) :2033-2037
[9]   Processing of carbon-fiber reinforced (SiC plus ZrC) mini-composites by soft-solution approach and their characterization [J].
Padmavathi, N. ;
Kumari, Sweety ;
Prasad, V. V. Bhanu ;
Subrahmanyam, J. ;
Ray, K. K. .
CERAMICS INTERNATIONAL, 2009, 35 (08) :3447-3454
[10]   Repeated thermal shock behavior of the ZrB2-SiC-ZrC ultrahigh-temperature ceramic [J].
Qi, Fei ;
Meng, Songhe ;
Guo, Hao .
MATERIALS & DESIGN, 2012, 35 :133-137