Effect of SiC/Si3N4 micro-reinforcement on mechanical and wear properties of friction stir welded AA6061-T6 aluminum alloy

被引:14
作者
Kumar, Nitesh [1 ]
Patel, Vinay Kumar [2 ]
机构
[1] Meerut Inst Engn & Technol, Dept Mech Engn, Meerut 250005, Uttar Pradesh, India
[2] Govind Ballabh Pant Inst Engn & Technol Ghurdauri, Dept Mech Engn, Pauri Garhwal 246194, Uttarakhand, India
来源
SN APPLIED SCIENCES | 2020年 / 2卷 / 09期
关键词
Friction stir welding; Mechanical properties; Silicon nitride; Silicon carbide; Aluminum alloy; SIC PARTICLE ADDITION; HEAT-TREATMENT; TEMPER CONDITION; WELDING PROCESS; MICROSTRUCTURE; BEHAVIOR; JOINTS; PARAMETERS; STRENGTH; HARDNESS;
D O I
10.1007/s42452-020-03381-y
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Friction stir welding (FSW) is extensively used to join aluminum alloys components for applications in structural, aviation and automotive sectors. In this investigation, the mechanical properties (tensile strength, percentage elongation, and microhardness), abrasive wear properties and microstructure of friction stir welded joint of AA6061-T6 were studied by inter-plate reinforcing of silicon carbide microparticles (mu SiC) and silicon nitride microparticles (mu Si3N4). The friction stir welding was performed at different tool rotational speed (TRS) (750, 1000 and 1400 rpm) and welding speed of 56, 80 and 112 mm/min. The friction stir welded joint without reinforcement and with mu SiC exhibited maximum tensile strength at two combinations of welding speed and tool rotational speed; one at welding speed of 112 mm/min, TRS of 1000 RPM and other at welding speed of 56 mm/min and TRS of 1400 rpm. It was realized that the reinforcement of mu SiC and mu Si3N4 decreased the tensile properties of the welded joint but improved the abrasive wear and microhardness properties considerably in the stir zone. The reinforcement of mu SiC during FSW demonstrated better tensile, microhardness and abrasive wear resistant properties than the FSW joints with mu Si3N4 reinforcement. The improvement in microhardness of the FSW joint reinforced with SiC and Si3N4 microparticles is attributed to the pinning effect produced by the hard particles inclusions.
引用
收藏
页数:11
相关论文
共 37 条
[1]   The Effect of SiC Particle Addition During FSW on Microstructure and Mechanical Properties of AZ31 Magnesium Alloy [J].
Abbasi, M. ;
Abdollahzadeh, A. ;
Bagheri, B. ;
Omidvar, H. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (12) :5037-5045
[2]  
[Anonymous], 2020, MATER TODAY-PROC, DOI DOI 10.1016/J.MATPR.2019.09.220
[3]  
[Anonymous], 2013, ASTMC642
[4]  
[Anonymous], 2019, J PHYS C SER, DOI DOI 10.1088/1742-6596/1240/1/012164
[5]  
[Anonymous], 2020, MATER TODAY PROC 4, DOI DOI 10.1016/J.MATPR.2019.05.466
[6]   Mechanical Characteristics of Welded Joints of Aluminum Alloy 6061 T6 Formed by Arc and Friction Stir Welding [J].
Astarita, A. ;
Squillace, A. ;
Nele, L. .
METAL SCIENCE AND HEAT TREATMENT, 2016, 57 (9-10) :564-569
[7]   Theoretical and experimental investigation into friction stir welding of AA 5086 [J].
Aval, H. Jamshidi ;
Serajzadeh, S. ;
Kokabi, A. H. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2011, 52 (5-8) :531-544
[8]   Effect of post-weld heat treatment on the mechanical behavior and dislocation density of friction stir welded Al6061 [J].
Baghdadi, Amir Hossein ;
Rajabi, Armin ;
Selamat, Nor Fazilah Mohamad ;
Sajuri, Zainuddin ;
Omar, Mohd Zaidi .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 754 :728-734
[9]   Relationship between base metal properties and friction stir welding process parameters [J].
Balasubramanian, V. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 480 (1-2) :397-403
[10]   Friction stir welded structural materials: beyond Al-alloys [J].
Cam, G. .
INTERNATIONAL MATERIALS REVIEWS, 2011, 56 (01) :1-48