Eco-friendly composites based on ceramic tiles industrial wastes and acrylonitrile butadiene rubber

被引:16
作者
Abd-El Messieh, Salwa L. [1 ]
Rozik, Nehad N. [2 ]
Youssef, Nadia F. [3 ]
机构
[1] NRC, Microwave Phys & Dielect Dept, Giza, Egypt
[2] NRC, Polymer & Pigments Dept, Giza, Egypt
[3] Housing & Bldg Natl Res Ctr HBRC, Raw Bldg Mat Technol & Proc Res Inst, Giza, Egypt
关键词
DIELECTRIC-PROPERTIES; SOLID-WASTES; RELAXATION; MIXTURES;
D O I
10.1002/pc.24686
中图分类号
TB33 [复合材料];
学科分类号
摘要
Ceramic floor tile production lines commonly produce two types of waste: ground fired biscuit waste of ceramic tiles (WGB) and ground glazed fired floor tiles waste (WGF). These two wastes come from the same starting alumina silicate base materials but differ in thermal treatments (further firing) and surface treatments (glazing). These waste ceramics were ground into fine powders and evaluated as potential fillers for acrylonitrile butadiene rubber (NBR). The raw ceramic powders were investigated through X-ray diffraction, X-ray fluorescence, and laser scattering techniques. Particulate composites consisting of an NBR matrix with ceramic filler contents of 5, 10, 15, 20, 30, 40, and 50% were prepared in the form of cubes and discs. Scanning electron microscopy was used to determine the filler distribution inside NBR matrix. Electrical, mechanical, and thermal properties were also investigated. The electrical permittivity epsilon ' and the dielectric loss epsilon '' were found to be higher in the case of NBR/WGB than those measured for NBR/WGF at the same filler content. The mechanical properties follow the same trend as that of the electrical properties. The thermal stability of 5 and 40% concentrations were studied and the results indicate that the WGB loaded samples showed higher thermal stability than the samples loaded with WGF. Finally, the utilization of these ground waste ceramics as fillers for NBR was recommended due to improvements in electrical insulation, antistatic behavior, and thermal stability, especially for the Biscuit waste. Note that at the 30 wt% concentration for both fillers in NBR, results in composites that fulfill the targets of economical and environmental goals. POLYM. COMPOS., 40:544-552, 2019. (c) 2017 Society of Plastics Engineers
引用
收藏
页码:544 / 552
页数:9
相关论文
共 27 条
[1]   Effect of curing time and sulfur content on the dielectric relaxation of styrene butadiene rubber [J].
Abd-El-Messieh, SL ;
Abd-El-Nour, KN .
JOURNAL OF APPLIED POLYMER SCIENCE, 2003, 88 (07) :1613-1621
[2]  
AbdelMessieh SL, 1996, J APPL POLYM SCI, V62, P805, DOI 10.1002/(SICI)1097-4628(19961031)62:5<805::AID-APP13>3.0.CO
[3]  
2-R
[4]   DIELECTRIC-PROPERTIES OF SOME SYNTHETIC RUBBER MIXTURES .2. BUTYL RUBBER CARBON-BLACK MIXTURES [J].
ABDELNOUR, KN ;
HANNA, FF ;
ABDELMESSIEH, SL .
POLYMER DEGRADATION AND STABILITY, 1992, 35 (02) :121-124
[5]  
Amin SK., 2016, Int J Appl Eng Res, V11, P2680, DOI DOI 10.1016/J.CONBUILDMAT.2015.03.028
[6]  
[Anonymous], 2011, 430R11005 EPA
[7]  
[Anonymous], 2012, 130062012 ISO
[8]  
[Anonymous], 31672015 ES
[9]  
EEAA, 2002, CONTR IND POLL PROJ, P5
[10]  
El-Fadaly E., 2010, J AM SCI, V6, P224