Integration of metallic endoprotheses in dog femur studied by near-infrared Fourier-transform Raman microscopy

被引:11
作者
Döpner, S
Müller, F
Hildebrandt, P
Müller, RT
机构
[1] Max Planck Inst Strahlenchem, D-45470 Mulheim, Germany
[2] Univ Essen Gesamthsch Klinikum, Orthopad Klin & Poliklin, D-45122 Essen, Germany
关键词
Raman microscope; NIR-FT Raman; component analysis; bone mineralization; hydroxyapatite coating;
D O I
10.1016/S0142-9612(01)00252-6
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The integration of hydroxyapatite-coated implants in dog femur was studied by near-infrared Fourier-transform Raman microscopy. Raman spectra were taken in lateral scans in step widths of 10-40 mum from the implant surface up to a distance of 320 pin into the bone tissue. The spectra were subjected to a component analysis for the quantitative determination of the protein and the inorganic components. This quantitative analysis is shown to be more reliable than conventional band fitting procedures and allows, for the first time, the quantitative distinction between the hydroxyapatite form of mature bone tissue and synthetic hydroxyapatite introduced by the implant coating. It is demonstrated that Full mineralization of the ongrowing bone is not achieved after 6 months, In contrast, after a residence time of 18 months in the body, the Raman spectra reveal a complete calcification of the new bone tissue as indicated by content of biological hydroxyapatite that is the same as in mature bone tissue throughout the whole implant/bone interface. On the other hand, the content of synthetic hydroxyapatite is strongly reduced in the sample prepared after eighteen months implantation whereas for the shorter implantation time, substantial contributions of synthetic hydroxyapatite are found even at positions beyond the thickness of the implant coating. These results indicate that the coating material is actively involved in the mineralization of ongrowing bone. Possible mechanisms for the underlying transport processes in the implant/bone interface are discussed. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1337 / 1345
页数:9
相关论文
共 31 条
[1]  
BARTOLOMAI G, 1975, SPEKTROSKOPISCHE MOD
[2]   EFFECT OF CALCIUM-PHOSPHATE (CA-P) COATINGS ON TRABECULAR BONE RESPONSE - A HISTOLOGICAL STUDY [J].
CAULIER, H ;
VANDERWAERDEN, JPCM ;
PAQUAY, YCGJ ;
WOLKE, JGC ;
KALK, W ;
NAERT, I ;
JANSEN, JA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1995, 29 (09) :1061-1069
[3]  
COLLIER JP, 1992, CLIN ORTHOP RELAT R, P97
[4]   CRYSTAL DISSOLUTION OF BIOLOGICAL AND CERAMIC APATITES [J].
DACULSI, G ;
LEGEROS, RZ ;
MITRE, D .
CALCIFIED TISSUE INTERNATIONAL, 1989, 45 (02) :95-103
[5]  
Dippel B, 1998, BIOSPECTROSCOPY, V4, P403, DOI 10.1002/(SICI)1520-6343(1998)4:6<403::AID-BSPY5>3.0.CO
[6]  
2-M
[7]   Development of an inverted NIR-FT-Raman microscope for biomedical applications [J].
Dippel, B ;
Tatsch, E ;
Schrader, B .
JOURNAL OF MOLECULAR STRUCTURE, 1997, 408 :247-251
[8]  
DOPNER S, 1996, SPECTROCHIM ACTA A, V51, P573
[9]   BONDING OF HYDROXYAPATITE-COATED FEMORAL PROSTHESES - HISTOPATHOLOGY OF SPECIMENS FROM 4 CASES [J].
HARDY, DCR ;
FRAYSSINET, P ;
GUILHEM, A ;
LAFONTAINE, MA ;
DELINCE, PE .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1991, 73 (05) :732-740
[10]   Total hip arthroplasty with hydroxyapatite-coated prostheses [J].
Jaffe, WL ;
Scott, DF .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1996, 78A (12) :1918-1934