LOW-TEMPERATURE NITRIDING BEHAVIOR OF COMPRESSIVE DEFORMED AISI 316Ti AUSTENITIC STAINLESS STEELS

被引:3
作者
Kahraman, Fatih [1 ]
Gencer, Goke Mehmet [1 ]
Kahraman, Ayca D. [2 ]
Yolcu, Coskun [1 ]
Kahraman, Haydar [3 ]
机构
[1] Dokuz Eylul Univ, Engn Fac, Mech Engn Dept, Izmir, Turkey
[2] Manisa Celal Bayar Univ, Engn Fac, Mech Engn Dept, Manisa, Turkey
[3] Dokuz Eylul Univ, Engn Fac, Metalurg & Mat Engn Dept, Izmir, Turkey
关键词
Low-temperature nitriding; quasi-static deformation; chromium nitride (CrN); compound layer; AISI 316Ti stainless steel; PLASTIC-DEFORMATION; CYCLIC DEFORMATION; SHEAR BANDS; PLASMA; MARTENSITE; MICROSTRUCTURES; MECHANISMS; FATIGUE; 304L;
D O I
10.1142/S0218625X18501883
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of compressive cold deformation under the quasi-static loads on the nitride formation, nitride layer growth and surface hardness properties were researched in this study. Martensite structure did not form in AISI 316Ti stainless steel as a result of quasi-static deformation. Diffusion layer did not form in all nitrided samples. Both the deformed and undeformed samples have only compound layer on the surfaces at the low-temperature nitriding conditions (400 degrees C, 7h). According to the X-ray diffraction (XRD), energy-dispersive spectroscopy (EDS) and electron probe microanalysis (EPMA) results, S-phase and chromium nitride (CrN) were formed in the compound layers of the deformed samples. However, CrN did not form in the compound layer of the undeformed sample. The optical microscope (OM) results showed that the compressive cold deformation increased the nitrogen diffusion rate and led to thicker nitrided layer than the undeformed sample under the same plasma-nitriding conditions. All nitrided layers presented higher microhardness values ( similar to 1200 HV) when compared with the untreated sample hardness. It was also verified that the deformation amount did not affect significantly the nitrided layer hardness.
引用
收藏
页数:8
相关论文
共 43 条
  • [41] Wear Resistance and Non-Magnetic Layer Formation on 316L Implant Material with Plasma Nitriding
    Yetim, Ali Fatih
    Yazici, Mustafa
    [J]. JOURNAL OF BIONIC ENGINEERING, 2014, 11 (04) : 620 - 629
  • [42] Effect of dynamic plastic deformation on microstructure and annealing behaviour of modified 9Cr-1Mo steel
    Zhang, Z. B.
    Mishin, O. V.
    Tao, N. R.
    Pantleon, W.
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2015, 31 (06) : 715 - 721
  • [43] [No title captured]