Wear mechanism in contact tube

被引:17
作者
Shimizu, H
Yokota, Y
Mizuno, M
Kurokawa, T
机构
[1] Welding Co, Kobe Steel Ltd, Tech Dev Dept, Fujisawa, Kanagawa 2518551, Japan
[2] Kobe Steel Ltd, Tech Dev Grp, Thin Film Res Sect, Elect Res Lab,Nishi Ku, Kobe, Hyogo 6512271, Japan
关键词
contact tube; copper coating; electrical contact resistance; voltage drop; wear property; welding wire;
D O I
10.1179/174329306X77885
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stable sliding contact is the most important factor in the stable arc discharge of solid wire. If the contact tube wears seriously, arc discharge will become unstable and the wire position will be shifted. Ordinary non-Cu-coated solid wire causes much wear of the contact tube, about 10 times that caused by Cu-coated solid wire. The mechanism of contact tube wear is not only friction at high temperature, but also a molten bridge formed between the contact tube and wire surface. A complex of superfine particles decreases the amount of contact tube wear. For example, the mixture of graphite and magnetite reduces the amount of contact tube wear by 80%. These particles form an interface layer on the inner surface of the contact tube, and the layer prevents the transfer of molten Cu to the wire surface. The interface layer mainly consists of FeO and complex oxides.
引用
收藏
页码:94 / 105
页数:12
相关论文
共 19 条
[1]  
DENALE R, 1986, WELD J, V65, P28
[2]  
HOLM R, 2000, ELECT CONTACTS
[3]  
Kohno A, 1996, J JPN SOC TRIBOLOGIS, V41, P535
[4]  
MATSUI H, 1995, 119 PHYS ARC WELD RE
[5]  
NAGASAWA H, 1987, LUBRICANT, V32, P268
[6]  
NAGASAWA H, 1988, LUBRICANT, V33, P502
[7]  
ODA O, 1984, J JAPAN SOC MECH ENG, V87, P1252
[8]  
QUINN TP, 1995, WELD J, V74, pS115
[9]  
Samsonovin G. V., 1973, OXIDE HDB, P271
[10]  
SHIMIZU H, 2001, IIW DOCUMENT, V1681, P221