The present work demonstrates the synthesis of Cu-10 wt% TiB2 composites with a theoretical density of more than 90% by tailoring the spark plasma sintering (SPS) conditions in the temperature range of 400-700 degrees C. Interestingly, 10 wt% Pb addition to Cu-10 wt% TiB2 lowers the sinter density and the difference in the densification behavior of the investigated compositions was discussed in reference to the current profile recorded during a SPS cycle. The sintering kinetics and phase assemblage were also discussed in reference to surface melting of the constituents prior to bulk melting temperature, temperature dependent wettability of Pb on Cu, diffusion kinetics of Cu as well as the formation of various oxides. An important result is that a high hardness of around 2 GPa and relative density close to 92% qtheoretical was achieved for the Cu-10 wt% TiB2-10 wt% Pb composite, and such a combination has never been achieved before using any conventional processing route.
引用
收藏
页码:1517 / 1528
页数:12
相关论文
共 50 条
  • [1] Fretting wear study of Cu-10 wt% TiB2 and Cu-10 wt% TiB2-10 wt% Pb composites
    Sharma, Amit S.
    Mishra, Nisha
    Biswas, Krishanu
    Basu, Bikramjit
    WEAR, 2013, 306 (1-2) : 138 - 148
  • [2] Densification kinetics, phase assemblage and hardness of spark plasma sintered Cu–10 wt% TiB2 and Cu–10 wt% TiB2–10 wt% Pb composites
    Amit S. Sharma
    Nisha Mishra
    Krishanu Biswas
    Bikramjit Basu
    Journal of Materials Research, 2013, 28 : 1517 - 1528
  • [3] Martensite aging kinetics in the Cu-10 wt.%Al and Cu-10 wt.%Al-10 wt.%Ag alloys
    A. T. Adorno
    R. A. G. Silva
    Journal of Materials Science, 2008, 43 : 1087 - 1093
  • [4] Martensite aging kinetics in the Cu-10 wt.%Al and Cu-10 wt.%Al-10 wt.%Ag alloys
    Adorno, A. T.
    Silva, R. A. G.
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (03) : 1087 - 1093
  • [5] Spark Plasma Sintering of Nanocrystalline Cu and Cu-10 Wt Pct Pb Alloy
    Sharma, Amit S.
    Biswas, Krishanu
    Basu, Bikramjit
    Chakravarty, Dibyendu
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (07): : 2072 - 2084
  • [6] Spark Plasma Sintering of Nanocrystalline Cu and Cu-10 Wt Pct Pb Alloy
    Amit S. Sharma
    Krishanu Biswas
    Bikramjit Basu
    Dibyendu Chakravarty
    Metallurgical and Materials Transactions A, 2011, 42 : 2072 - 2084
  • [7] Ageing behavior in the Cu-10 wt.%Al and Cu-10 wt.%Al-4 wt.%Ag alloys
    Adorno, A. T.
    Silva, R. A. G.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 473 (1-2) : 139 - 144
  • [8] Reverse martensitic transformation in the Cu-10 wt% Al-6 wt%Ag alloy
    Adorno, AT
    Silva, RAG
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (23) : 6217 - 6221
  • [9] Reverse martensitic transformation in the Cu-10 wt% Al-6 wt%Ag alloy
    A. T. Adorno
    R. A. G. Silva
    Journal of Materials Science, 2005, 40 : 6217 - 6221
  • [10] Effect of Ag addition on the martensitic phase of the Cu-10 wt.% Al alloy
    Silva, R. A. G.
    Cuniberti, A.
    Stipcich, M.
    Adorno, A. T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 456 (1-2): : 5 - 10