Physicochemical studies of mild steel corrosion and atmospheric corrosivity mapping of Karachi: An important harbor city of modern Maritime Silk Route

被引:10
作者
Zafar, Faiza [1 ]
Bano, Humaira [1 ]
Mahmood, Azhar [2 ]
Corvo, Francisco [3 ]
Rodriguez, Joelis [4 ]
机构
[1] Univ Karachi, Dept Chem, Karachi 75270, Pakistan
[2] Natl Univ Sci & Technol, Sch Nat Sci, Islamabad, Pakistan
[3] Autonomous Univ Campeche, Corros Res Ctr, Campeche, Mexico
[4] Res Ctr Appl Chem CIQA, Adv Mat Dept, Saltillo, Coahuila, Mexico
来源
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION | 2020年 / 71卷 / 09期
关键词
corrosivity map; Fourier-transform infrared spectroscopy; mild steel; scanning electron microscopy; X-ray diffraction; CARBON-STEEL; AIR-POLLUTION; COASTAL AREAS; KINETICS; ZINC; ALUMINUM; EXPOSURE; COPPER; IMPACT;
D O I
10.1002/maco.202011793
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper has reported physicochemical features of mild steel's corrosion products and provided atmospheric corrosivity maps of Karachi harbor city, drafted on the basis of spatial distribution of corrosion data from July 2018 to June 2019 at 10 different urban, industrial, and marine test sites. Exposure tests have been performed to study atmospheric corrosivity, corrosion products, and corrodants including chloride, sulfur dioxide, time of wetness (TOW), and corrosion rate as per ISO and ASTM standards. Scanning electron microscope, Fourier-transform infrared spectroscopy, and X-ray diffraction have corroborated the presence of lepidocrocite, goethite, magnetite, and quartz phases at almost all the test sites, with slight variations in their morphologies and quantities. The data analysis has revealed that TOW is a major detrimental factor to accelerate corrosion of mild steel at Karachi city. The corrosivity category of all urban and marine test sites is found in C-4-C-5 range, whereas for industrial test sites, it is found in C-3-C-5 range. Resultant corrosivity maps have shown that the prevailing atmosphere is significantly corrosive at Karachi harbor city. This study has furnished a novel product of atmospheric corrosivity map, which is the first-ever corrosivity map for Pakistan.
引用
收藏
页码:1557 / 1575
页数:19
相关论文
共 34 条
  • [1] Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel
    Alcantara, J.
    Chico, B.
    Diaz, I.
    de la Fuente, D.
    Morcillo, M.
    [J]. CORROSION SCIENCE, 2015, 97 : 74 - 88
  • [2] [Anonymous], 2003, STANDARD PRACTICE PR
  • [3] [Anonymous], 2012, ISO 9223:2012
  • [4] [Anonymous], 1992, Corrosion of metals and alloys-corrosivity of atmospheres-classification
  • [5] [Anonymous], 2003, STANDARD PRACTICE CO
  • [6] Balasubramaniam R, 2003, CURR SCI INDIA, V85, P1546
  • [7] Bano H., 2015, INT J ADV RES, V4, P318
  • [8] Atmospheric corrosion study in a harbor located in a tropical island
    Castaneda, Abel
    Valdes, Cecilia
    Corvo, Francisco
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (10): : 1462 - 1477
  • [9] Atmospheric corrosion of carbon steel in Colombia
    Castano, J. G.
    Botero, C. A.
    Restrepo, A. H.
    Agudelo, E. A.
    Correa, E.
    Echeverria, F.
    [J]. CORROSION SCIENCE, 2010, 52 (01) : 216 - 223
  • [10] Corrosivity maps of Spain for zinc in rural atmospheres
    Chico, B.
    de la Fuente, D.
    Vega, J. M.
    Morcillo, M.
    [J]. REVISTA DE METALURGIA, 2010, 46 (06) : 485 - 492