Effects of loading rates on mode I interlaminar fracture toughness of carbon/epoxy composite toughened by carbon nanotube films

被引:55
作者
Li, Zhouyi [1 ]
Wang, Yu [1 ]
Cao, Junchao [1 ]
Meng, Xianghao [1 ]
Aamir, Raza Muhammad [1 ]
Lu, Weibang [4 ]
Suo, Tao [1 ,2 ,3 ]
机构
[1] Northwestern Polytech Univ, Sch Aeronaut, Xian 710072, Shaanxi, Peoples R China
[2] Northwestern Polytech Univ, Joint Int Res Ctr Impact Dynam & Its Engn Applica, Xian 710072, Shaanxi, Peoples R China
[3] Northwestern Polytech Univ, Shaanxi Key Lab Impact Dynam & Engn Applicat IDEA, Xian 710072, Shaanxi, Peoples R China
[4] Suzhou Inst Nanotech & Nanobion, Suzhou 215123, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Carbon nanotubes; Composites; Interlaminar fracture toughness; Impact behavior; Morphology; MECHANICAL-PROPERTIES; FIBER; BEHAVIOR; COMPRESSION; IMPROVEMENT; DAMAGE; CFRPS;
D O I
10.1016/j.compositesb.2020.108270
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Carbon fiber reinforced resin matrix composites were toughened by the continuous and randomly distributed carbon nanotubes (CNTs), which were fabricated by floating catalytic chemical vapor deposition (FCCVD) method. Toughening was achieved by deploying CNT film of different a real density as interleaves in the carbon fiber reinforced composites. Double cantilever beam (DCB) specimens were adopted in both quasi-static and dynamic fracture tests. The electromagnetic Hopkinson bar was applied to achieve pure type I fracture mode at high loading speeds of 15 m/s and 24 m/s. The effects of CNTs and loading rates on the Mode I fracture toughness of the composites are investigated. It is shown that fracture toughness approaches a maximum value of 626 J/m(2) under quasi-static loading, only if a 2-layered CNT film is being applied as an interleave, which is twice that of the neat composite (without CNT interleaves). Under dynamic loading, all the specimens either with or without CNTs show increases in the fracture toughness with the increase in loading rate. Different from the results of quasi-static tests, under dynamic loading conditions, the fracture toughness increases monotonously and approaches to a maximum value of 1380 J/m(2) when 40-layered CNT film was applied, which is a remarkable increase of 140% if compared with that of the neat specimen. A detailed analysis of mechanisms responsible for the ameliorating effects of CNTs interleaves is carried out. It is believed that strengthening of interfaces between carbon fibers and matrix, deformation of resin and detachment of CNTs from the matrix are the main factors responsible for this effect.
引用
收藏
页数:19
相关论文
共 35 条
[1]   Improvement of the mode I interlaminar fracture toughness of carbon fiber; composite reinforced with electrospun nylon nanofiber [J].
Aljarrah, Mohannad T. ;
Abdelal, Nisrin R. .
COMPOSITES PART B-ENGINEERING, 2019, 165 :379-385
[2]  
[Anonymous], [No title captured]
[3]   The fracture behaviour of structural adhesives under high rates of testing [J].
Blackman, B. R. K. ;
Kinloch, A. J. ;
Sanchez, F. S. Rodriguez ;
Teo, W. S. ;
Williams, J. G. .
ENGINEERING FRACTURE MECHANICS, 2009, 76 (18) :2868-2889
[4]   Characterization of carbon nanotube enhanced interlaminar fracture toughness of woven carbon fiber reinforced polymer composites [J].
Chaudhry, M. S. ;
Czekanski, A. ;
Zhu, Z. H. .
INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2017, 131 :480-489
[5]   Nanofibre bridging as a toughening mechanism in carbon/epoxy composite laminates interleaved with electrospun polyamide nanofibrous veils [J].
Daelemans, Lode ;
van der Heijden, Sam ;
De Baere, Ives ;
Rahier, Hubert ;
Van Paepegem, Wim ;
De Clerck, Karen .
COMPOSITES SCIENCE AND TECHNOLOGY, 2015, 117 :244-256
[6]  
[杜善义 DU Shanyi], 2008, [复合材料学报, Acta Materiae Compositae Sinica], V25, P1
[7]   Mode II delamination and damage resistance of carbon/epoxy composite laminates interleaved with thermoplastic particles [J].
Gao, Feng ;
Jiao, Guiqiong ;
Lu, Zhixian ;
Ning, Rongchang .
JOURNAL OF COMPOSITE MATERIALS, 2007, 41 (01) :111-123
[8]   Pull-out performance of rectangular z-pins in hot-cured carbon fiber reinforced laminates [J].
Hoffmann, Julian ;
Scharr, Gerhard .
COMPOSITE STRUCTURES, 2018, 186 :62-67
[9]   Effect of the loading rate on mode I interlaminar fracture toughness of laminated composites [J].
Hug, G. ;
Thevenet, P. ;
Fitoussi, J. ;
Baptiste, D. .
ENGINEERING FRACTURE MECHANICS, 2006, 73 (16) :2456-2462
[10]   HELICAL MICROTUBULES OF GRAPHITIC CARBON [J].
IIJIMA, S .
NATURE, 1991, 354 (6348) :56-58