Green synthesis of Ni supported hematite catalysts for syngas production from catalytic cracking of toluene as a model compound of biomass tar

被引:39
作者
Zou, Xuehua [1 ]
Ma, Zhiyuan [1 ]
Liu, Haibo [1 ]
Chen, Dong [1 ]
Wang, Can [1 ]
Zhang, Ping [2 ]
Chen, Tianhu [1 ]
机构
[1] Hefei Univ Technol, Sch Resources & Environm Engn, Lab Nanomineral & Environm Mat, Hefei 230009, Anhui, Peoples R China
[2] Guangzhou Inst Energy Testing, Guangzhou 510170, Guangdong, Peoples R China
基金
中国国家自然科学基金;
关键词
Tar; Hematite; Ni-Fe alloy; Lattice oxygen; Catalytic cracking; CHEMICAL-LOOPING COMBUSTION; IRON-ALUMINA CATALYSTS; FLUIDIZED-BED REACTOR; OXYGEN CARRIER; COKE FORMATION; SYNTHESIS GAS; GASIFICATION; CARBON; METHANE; PERFORMANCE;
D O I
10.1016/j.fuel.2017.12.063
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
In this work, natural limonite (NL) was selected as the precursor of hematite (H) to prepare the Ni-based catalysts (Nix/H) for catalytic cracking of toluene. The influences of nickel loading and reaction temperature on catalytic cracking of toluene as well as the lifetime of catalyst were evaluated and the gas products were determined. The catalysts before and after catalytic cracking were characterized by XRD (X-ray diffraction), H-2-TPR (H-2 temperature-programmed reduction), TEM (Transmission electron microscopy), XPS (X-ray photoelectron spectroscopy). The results showed that the catalytic activity of Nix/H was obviously improved after the Ni addition due to the formation of Ni-Fe alloy. Toluene conversion increased at first with increasing of Ni loading from 0 to 6% and then decreased from 6 to 10%. High toluene conversion of 96% and stability were achieved as the Ni loading was 6% at the reaction temperature of 800 degrees C. Meanwhile, toluene was mainly decomposed into CO, H-2, CH4, CO2 and hematite was transformed into magnetite due to the consumption of active lattice oxygen during the catalytic cracking reaction. However, the decrease in catalytic activity of Nix/H with the increase of reaction time should be attributed to the metal carbide type coke formation.
引用
收藏
页码:343 / 351
页数:9
相关论文
共 40 条
  • [21] Thermal treatment of natural goethite: Thermal transformation and physical properties
    Liu, Haibo
    Chen, Tianhu
    Zou, Xuehua
    Qing, Chengsong
    Frost, Ray L.
    [J]. THERMOCHIMICA ACTA, 2013, 568 : 115 - 121
  • [22] Characterization and catalytic performance of Fe3Ni8/palygorskite for catalytic cracking of benzene
    Liu, Haibo
    Chen, Tianhu
    Chang, Dongyin
    Chen, Dong
    He, Hongping
    Yuan, Peng
    Xie, Jingjing
    Frost, Ray L.
    [J]. APPLIED CLAY SCIENCE, 2013, 74 : 135 - 140
  • [23] Catalytic cracking of tar derived from rice hull gasification over palygorskite-supported Fe and Ni
    Liu, Haibo
    Chen, Tianhu
    Chang, Dongyin
    Chen, Dong
    He, Hongping
    Frost, Ray L.
    [J]. JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2012, 363 : 304 - 310
  • [24] Effect of preparation method of palygorskite-supported Fe and Ni catalysts on catalytic cracking of biomass tar
    Liu, Haibo
    Chen, Tianhu
    Chang, Dongyin
    Chen, Dong
    Kong, Dejun
    Zou, Xuehua
    Frost, Ray L.
    [J]. CHEMICAL ENGINEERING JOURNAL, 2012, 188 : 108 - 112
  • [25] Use of an Fe-Based Residue from Alumina Production as an Oxygen Carrier in Chemical-Looping Combustion
    Mendiara, T.
    Abad, A.
    de Diego, L. F.
    Garcia-Labiano, F.
    Gayan, P.
    Adanez, J.
    [J]. ENERGY & FUELS, 2012, 26 (02) : 1420 - 1431
  • [26] Steam reforming of biomass gasification tar using benzene as a model compound over various Ni supported metal oxide catalysts
    Park, Hyun Ju
    Park, Sung Hoon
    Sohn, Jung Min
    Park, Junhong
    Jeon, Jong-Ki
    Kim, Seung-Soo
    Park, Young-Kwon
    [J]. BIORESOURCE TECHNOLOGY, 2010, 101 : S101 - S103
  • [27] Pore geometry influence on the deactivation behavior of Ni-based catalysts for simultaneous production of hydrogen and nanocarbon
    Salmones, J.
    Wang, J. A.
    Valenzuela, M. A.
    Sanchez, E.
    Garcia, A.
    [J]. CATALYSIS TODAY, 2009, 148 (1-2) : 134 - 139
  • [28] Recent progresses in catalytic tar elimination during biomass gasification or pyrolysis-A review
    Shen, Yafei
    Yoshikawa, Kunio
    [J]. RENEWABLE & SUSTAINABLE ENERGY REVIEWS, 2013, 21 : 371 - 392
  • [29] Study on coke formation over Ni/γ-Al2O3, Co-Ni/γ-Al2O3, and Mg-Co-Ni/γ-Al2O3 catalysts for carbon dioxide reforming of methane
    Son, In Hyuk
    Lee, Seung Jae
    Song, In Yong
    Jeon, Woo Sung
    Jung, Insun
    Yun, Dong Jin
    Jeong, Dae-Woon
    Shim, Jae-Oh
    Jang, Won-Jun
    Roh, Hyun-Seog
    [J]. FUEL, 2014, 136 : 194 - 200
  • [30] Song T, 2016, INT J GREENH GAS CON, V11, P326