Powder injection molding of Ti-6Al-4V alloy

被引:67
作者
Guo, SB [1 ]
Qu, XH
He, XB
Zhou, T
Duan, BH
机构
[1] Jiangxi Sci & Technol Normal Univ, Jiangxi Key Lab Surface Engn, Nanchang 330013, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
关键词
PIM; Ti-6Al-4V; carbon and oxygen control; mechanical properties;
D O I
10.1016/j.jmatprotec.2005.12.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An improved wax-based binder was developed for the powder injection molding of Ti-6Al-4V. A critical powder loading of 72 vol% and a pseudo-plastic flow behavior were obtained by the feedstock based on the binder. The injection molding, debinding and sintering processes were studied. An ideal control of carbon and oxygen contents was achieved by thermal debinding in vacuum atmosphere (10(-3) Pa). The mechanical properties of as-sintered specimens were almost equivalent to those of the same alloy made by conventional press-sintefing process. Good shape retention and +/- 0.02 mm dimension deviation were achieved. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:310 / 314
页数:5
相关论文
共 12 条
[1]  
Froes FH, 2000, MATER TECHNOL, V15, P295
[2]  
FROES FH, 2001, ADV POWDER METALL M, P1298
[3]  
German R. M., 1999, MPR, V54, P24
[4]  
GERMAN RM, 1991, APPL MECH REV, V44, P134
[5]  
Kato K., 1999, J JPN SOC POWDER POW, V46, P865, DOI DOI 10.2497/JJSPM.46.865
[6]  
KEI A, 1989, ADV POWDER METALL, V3, P121
[7]  
LANE PD, 1994, MPR, V49, P22
[8]   Effect of carbon and oxygen on microstructure and mechanical properties of Ti-25V-15Cr-2Al (wt%) alloys [J].
Li, YG ;
Blenkinsop, PA ;
Loretto, MH ;
Rugg, D ;
Voice, W .
ACTA MATERIALIA, 1999, 47 (10) :2889-2905
[9]  
QU XH, 1998, CHINESE J NONFERROUS, V8, P436
[10]   Ti-6Al-4V/HA composite feedstock for injection molding [J].
Thian, ES ;
Loh, NH ;
Khor, KA ;
Tor, SB .
MATERIALS LETTERS, 2002, 56 (04) :522-532