Effect of aging treatments and microstructural evolution on corrosion resistance of tungsten substituted 2205 duplex stainless steel

被引:29
作者
Ahn, YS [1 ]
Kim, JM [1 ]
Jeong, BH [1 ]
机构
[1] Pukyong Natl Univ, Sch Mat Engn, Pusan 608739, South Korea
关键词
D O I
10.1179/026708302225001642
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of partial substitution of tungsten for molybdenum on the microstructure and corrosion resistance in 22Cr-5Ni-3Mo duplex stainless steel (DSS) has been investigated following aging heat treatments in a temperature range of 600-1000degreesC. Electrochemical tests were carried out for the evaluation of corrosion resistance. Aging treatment had hardly influenced the general corrosion resistance. With the increase of aging time, the pitting corrosion resistance of the DSSs had decreased. After aging for 2 min at 700-900degreesC, the pitting potential of the 3Mo steel decreased remarkably, while that of the W substituted steel hardly changed. During aging, the intermetallic sigma and secondary austenite (gamma(2)) phases were precipitated, and the pitting corrosion and intergranular corrosion resistance were significantly decreased after aging at 700-750degreesC for 10 h, which could be caused by the gamma(2) formation. The gamma(2) phase could effect the depletion of molybdenum and chromium in the gamma(2)/alpha and gamma(2)/sigma boundaries.
引用
收藏
页码:383 / 388
页数:6
相关论文
共 18 条
[1]   Effect of aging treatments on microstructure and impact properties of tungsten substituted 2205 duplex stainless steel [J].
Ahn, YS ;
Kang, JP .
MATERIALS SCIENCE AND TECHNOLOGY, 2000, 16 (04) :382-388
[2]  
CHARLES J, 1994, 4 INT P C DUPL STAIN, V1
[3]  
DEBOLD TA, 1992, J MET, V8, P685
[4]   THE APPLICABILITY OF DUPLEX STAINLESS-STEELS IN SOUR ENVIRONMENTS [J].
ERIKSSON, H ;
BERNHARDSSON, S .
CORROSION, 1991, 47 (09) :719-727
[5]  
Gunn R.N., 1997, DUPLEX STAINLESS STE, P14
[6]  
JOSEFSSON B, 1991, DUPLEX STAINLESS STE, P112
[7]  
MAEHARA Y, 1983, T IRON STEEL I JPN, V23, P240
[8]   THE DOUBLE LOOP REACTIVATION METHOD FOR DETECTING SENSITIZATION IN AISI-304 STAINLESS-STEELS [J].
MAJIDI, AP ;
STREICHER, MA .
CORROSION, 1984, 40 (11) :584-593
[9]   DETERMINATION OF THE MINIMUM SURFACE ENRICHMENT OF MOLYBDENUM REQUIRED TO INHIBIT ACTIVE DISSOLUTION OF AN FE-CR-NI-MO ALLOY [J].
NEWMAN, RC ;
FRANZ, EM .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1984, 131 (01) :223-225
[10]  
Nilsson J.-O., 1992, P C APPL STAINL STEE, P280