Hot cracking in pulsed Nd:YAG laser welding of AA5456

被引:49
作者
Hekmatjou, Hamidreza [1 ]
Naffakh-Moosavy, Homam [1 ]
机构
[1] TMU, Dept Mat Engn, POB 14115-143, Tehran, Iran
关键词
Aluminum alloy 5456; Laser welding; Pulsed Nd:YAG laser; Hot cracking; WROUGHT ALUMINUM-ALLOYS; PROGRESS;
D O I
10.1016/j.optlastec.2018.01.020
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
A 700 W pulsed Nd:YAG laser welding was employed to weld 5456 aluminum alloy plates with thickness of 5 mm. The weld penetration and tendency of liquation cracking in the heat affected zone and solidification cracking in the weld metal are investigated. It is found that hot cracks can be avoided by pulsed laser in preheated status. Increasing the laser average power in fixed pulse frequency and pulse duration resulted in a significant reduction in hot cracking tendency in pulsed laser welding. Also, the hot cracking susceptibility is reduced with increasing pulse frequency up to 50 Hz in fixed average power and pulse duration. The hot cracking tendency can be decreased by pulse duration decrement to 6 ms in fixed average power and pulse frequency. The factors contributing to the prevention or reduction of hot cracks in laser welding of aluminum alloy 5456 are the reduction in cooling rate causing change in solidification mode from columnar to equiaxed grains, and backfilling of liquated grain boundaries. With a 0.4 mm beam diameter Nd:YAG pulsed laser at 300 W average power, 6 ms pulse duration, 20 Hz pulse frequency, 5 mm/s travel speed and 150 degrees C preheating temperature, hot crack-free weld cross sections were achieved. (C) 2018 Elsevier Ltd. All rights reserved.
引用
收藏
页码:22 / 32
页数:11
相关论文
共 25 条
[1]  
Avallone U. A., 1987, MECH SOLIDS, V3, P2
[2]  
Cam G., 2013, SCI TECHNOL WELD JOI, P159
[3]   Analysis and Comparison of Friction Stir Welding and Laser Assisted Friction Stir Welding of Aluminum Alloy [J].
Campanelli, Sabina Luisa ;
Casalino, Giuseppe ;
Casavola, Caterina ;
Moramarco, Vincenzo .
MATERIALS, 2013, 6 (12) :5923-5941
[4]   Research and progress in laser welding of wrought aluminum alloys. II. Metallurgical microstructures, defects, and mechanical properties [J].
Cao, X ;
Wallace, W ;
Immarigeon, JP ;
Poon, C .
MATERIALS AND MANUFACTURING PROCESSES, 2003, 18 (01) :23-49
[5]   Research and progress in laser welding of wrought aluminum alloys. I. Laser welding processes [J].
Cao, X ;
Wallace, W ;
Poon, C ;
Immarigeon, JP .
MATERIALS AND MANUFACTURING PROCESSES, 2003, 18 (01) :1-22
[6]  
Clarke JA, 2001, ALUMINUM 2001: PROCEEDINGS OF THE TMS 2001 ANNUAL MEETING ALUMINUM AUTOMOTIVE AND JOINING SYMPOSIA, P117
[7]  
Ion J. C., 2013, SCI TECHNOL WELD JOI
[8]   The systematic parameter optimization in the Nd:YAG laser beam welding of Inconel 625 [J].
Jelokhani-Niaraki, M. R. ;
Arab, N. B. Mostafa ;
Naffakh-Moosavy, H. ;
Ghoreishi, M. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2016, 84 (9-12) :2537-2546
[9]  
Kanazawa H., 1997, J LIGHT MET WELD CON, V35, P10
[10]  
Kathuria Y. P., 2000, ACTA METALL SIN, V13, P49