Thermal stability of ultrafine grains in Al-Fe-Mn-Si foils prepared by ARB and subsequent rolling

被引:4
作者
Homola, P. [1 ]
Slamova, M. [1 ]
Slama, P. [1 ]
Cieslar, M. [1 ]
机构
[1] COMTES FHT Ltd, Dobrany 33441, Czech Republic
来源
NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2 | 2008年 / 584-586卷
关键词
thermal stability; accumulative roll bonding (ARB); Al-Fe-Mn-Si alloy; EBSD; TEM;
D O I
10.4028/www.scientific.net/MSF.584-586.905
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Accumulative Roll Bonding (ARB) is a severe plastic deformation process that allows producing ultrafine-grained materials (UFG). UFG sheets exhibit enhanced strength and very fine Brain structure. Foils used as fins in heat exchangers have to be very thin but must exhibit high strength combined with relatively high formability. Thus, materials produced using ARB may fulfil the exacting requirements on foil properties for such applications. The thermal stability of Al-Fe-Mn-Si foils produced using ARB and subsequent cold rolling was studied and compared with conventionally cold rolled (CCR) counterparts. The stability was assessed by isothermal annealing in the temperature range from 200 to 450 degrees C. Electron back scatter diffraction in a scanning electron microscope and transmission electron microscopy examinations of foils microstructure in the deformed and annealed states allowed the monitoring of structural changes. The magnitude of mechanical properties changes due to annealing was evaluated by microhardness measurements. Significant hardness increase was observed after annealing at 200 degrees C only in the ARB samples and was assigned to an annealing-induced hardening. The CCR foil exhibits higher non-recrystallized fraction and smaller mean lamellae boundary spacing in the temperature interval of 200-250 degrees C than ARB foils. The annealing at 450 degrees C results in identical hardness values and fully recrystallized microstructure of all foils, regardless the method used for their manufacturing. However, the ARB samples show higher stability of the refined substructure than their cold rolled counterparts due to continuous recrystallization occurring in the ARB foils.
引用
收藏
页码:905 / 910
页数:6
相关论文
共 34 条
  • [31] Relation between quenching wheel speed and microstructure, thermal stability and corrosion resistance of quinary Al-Ni-Y-Co-Si high entropy metallic glass ribbons prepared by melt spinning
    Zhang, Shuyan
    Zhang, Zhibin
    Chen, Changjiu
    Li, Xu
    Gao, Yangyang
    Liang, Xiubing
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2023, 601
  • [32] Relation between quenching wheel speed and microstructure, thermal stability and corrosion resistance of quinary Al-Ni-Y-Co-Si high entropy metallic glass ribbons prepared by melt spinning
    Zhang, Shuyan
    Zhang, Zhibin
    Chen, Changjiu
    Li, Xu
    Gao, Yangyang
    Liang, Xiubing
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2023, 601
  • [33] On the thermal stability of manganese(II) sulfate and its reaction with zeolite A to form the sodalite Na6Mn2[Al6Si6O24](SO4)2
    Warner, T. E.
    Bancells, M. M.
    Lund, P. Brilner
    Lund, F. W.
    Ravnsbaek, D. B.
    JOURNAL OF SOLID STATE CHEMISTRY, 2019, 277 : 434 - 440
  • [34] Characterisation of microstructure and thermal stability of rapidly solidified Al-8•5Fe-1•3V-1•7Si alloy during prolonged exposure at 625°C
    Solis-Ramos, E.
    Jones, H.
    Rainforth, W. M.
    MATERIALS SCIENCE AND TECHNOLOGY, 2006, 22 (11) : 1369 - 1379