Thermal stability of ultrafine grains in Al-Fe-Mn-Si foils prepared by ARB and subsequent rolling

被引:4
作者
Homola, P. [1 ]
Slamova, M. [1 ]
Slama, P. [1 ]
Cieslar, M. [1 ]
机构
[1] COMTES FHT Ltd, Dobrany 33441, Czech Republic
来源
NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2 | 2008年 / 584-586卷
关键词
thermal stability; accumulative roll bonding (ARB); Al-Fe-Mn-Si alloy; EBSD; TEM;
D O I
10.4028/www.scientific.net/MSF.584-586.905
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Accumulative Roll Bonding (ARB) is a severe plastic deformation process that allows producing ultrafine-grained materials (UFG). UFG sheets exhibit enhanced strength and very fine Brain structure. Foils used as fins in heat exchangers have to be very thin but must exhibit high strength combined with relatively high formability. Thus, materials produced using ARB may fulfil the exacting requirements on foil properties for such applications. The thermal stability of Al-Fe-Mn-Si foils produced using ARB and subsequent cold rolling was studied and compared with conventionally cold rolled (CCR) counterparts. The stability was assessed by isothermal annealing in the temperature range from 200 to 450 degrees C. Electron back scatter diffraction in a scanning electron microscope and transmission electron microscopy examinations of foils microstructure in the deformed and annealed states allowed the monitoring of structural changes. The magnitude of mechanical properties changes due to annealing was evaluated by microhardness measurements. Significant hardness increase was observed after annealing at 200 degrees C only in the ARB samples and was assigned to an annealing-induced hardening. The CCR foil exhibits higher non-recrystallized fraction and smaller mean lamellae boundary spacing in the temperature interval of 200-250 degrees C than ARB foils. The annealing at 450 degrees C results in identical hardness values and fully recrystallized microstructure of all foils, regardless the method used for their manufacturing. However, the ARB samples show higher stability of the refined substructure than their cold rolled counterparts due to continuous recrystallization occurring in the ARB foils.
引用
收藏
页码:905 / 910
页数:6
相关论文
共 34 条
  • [21] Formation of Al15Mn3Si2 Phase During Solidification of a Novel Al-12%Si-4%Cu-1.2%Mn Heat-Resistant Alloy and Its Thermal Stability
    Xiaojing Suo
    Hengcheng Liao
    Yiyun Hu
    Uday S. Dixit
    Pavel Petrov
    Journal of Materials Engineering and Performance, 2018, 27 : 2910 - 2920
  • [22] Formation of Al15Mn3Si2 Phase During Solidification of a Novel Al-12%Si-4%Cu-1.2%Mn Heat-Resistant Alloy and Its Thermal Stability
    Suo, Xiaojing
    Liao, Hengcheng
    Hu, Yiyun
    Dixit, Uday S.
    Petrov, Pavel
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (06) : 2910 - 2920
  • [23] The effect of metalloid content on glass forming ability, thermal stability and magnetic properties of Fe-Ta-Si-C powders prepared by mechanical alloying
    Yekta, Ehsan Bahadori
    Taghvaei, Amir Hossein
    Sharafi, Shahriyar
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 500 : 110 - 120
  • [24] Enhanced long-term thermal stability and mechanical properties of twin-roll cast Al-Mg-Si alloys with Mn and Cu additions
    Liu, Xu
    Ma, Yin-Long
    Wang, Xuan
    Zhang, Shao-You
    Zhang, Ming-Xue
    Wang, Hui-Yuan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 872
  • [25] The Thermal Stability and Elevated Temperature Mechanical Properties of Spray-Deposited SiCp/Al-11.7Fe-1.3V-1.7Si Composite
    Hao, L.
    He, Y. Q.
    Wang, Na
    Chen, Z. H.
    Chen, Z. G.
    Yan, H. G.
    Xu, Z. K.
    ADVANCED COMPOSITE MATERIALS, 2009, 18 (04) : 351 - 364
  • [26] Glass formation and magnetic study of new Fe70Ta5Si10C15 powders prepared by mechanical alloying with high thermal stability
    Yekta, Ehsan Bahadori
    Taghvaei, Amir Hossein
    Sharafi, Shahriar
    POWDER TECHNOLOGY, 2017, 322 : 241 - 249
  • [27] Effect of Transition Elements on the Thermal Stability of Glassy Alloys 82Al-16Fe-2TM (TM: Ti, Ni, Cu) Prepared by Mechanical Alloying
    Nguyen Thi Hoang Oanh
    Do Nam Binh
    Dung Dang Duc
    Quyen Hoang Thi Ngoc
    Nguyen Hoang Viet
    MATERIALS, 2021, 14 (14)
  • [28] Correlation between intercritical annealing duration and the tensile deformation behavior of Fe-7.5Mn-3.25Al-1Si-0.2C steels: Role of austenite stability, δ-ferrite, and texture
    Kumar, Deepak
    Sanyal, Souriddha
    Yadav, Mukesh Kumar
    Sen, Indrani
    Bandyopadhyay, Tapas Kumar
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1013
  • [29] Dual-phase Fe40Mn20Cr15Ti10Al10Ni5 high-entropy alloy prepared by mechanical alloying and spark plasma sintering: Alloying behavior, thermal stability, and mechanical properties
    Jain, Harsh
    Shadangi, Yagnesh
    Singh, Lalit Kumar
    Dubey, Ashutosh Kumar
    Mukhopadhyay, Nilay Krishna
    JOURNAL OF MATERIALS RESEARCH, 2025, 40 (01) : 123 - 139
  • [30] Thermal stability of ultrafine-grained structure produced by equal channel angular pressing in Fe-Mn-V-Ti-0.1C and Fe-Mo-Nb-V-0.1C low-carbon steels with various phase composition
    Mayer, G. G.
    Astafurova, E. G.
    Dobatkin, S. V.
    Naydenkin, E. V.
    Koshoina, V. S.
    Chumachenko, A. Yu.
    Belousova, N. S.
    OBRABOTKA METALLOV-METAL WORKING AND MATERIAL SCIENCE, 2013, (01): : 42 - 47