High-temperature fatigue behavior of a near-γ titanium aluminide alloy under isothermal and thermo-mechanical conditions

被引:32
作者
Christ, HJ [1 ]
Fischer, FOR
Maier, HJ
机构
[1] Univ Siegen, Inst Werkstofftechn, D-57068 Siegen, Germany
[2] Univ Paderborn, Lehrstuhl Werkstoffkunde, FB 10, D-33098 Paderborn, Germany
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2001年 / 319卷
关键词
near-gamma titanium aluminide; high-temperature fatigue; thermo-mechanical fatigue; environmental effect;
D O I
10.1016/S0921-5093(00)02013-X
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Fatigue tests were performed on smooth cylindrical specimens of a near-gamma titanium aluminide alloy with a duplex microstructure. The test temperature ranged from 500 to 750 degreesC in the isothermal tests and these temperatures were also used as minimum and maximum temperature of in-phase and out-of-phase thermo-mechanical fatigue (TMF) tests. Environmental degradation was studied running the experiments in air and high-vacuum. respectively, and the microstructural changes were characterized by transmission electron microscopy. Fatigue behavior was found to be strongly affected by temperature as a consequence of a change in the cyclic stress-strain response at approximate to 650 degreesC. At temperatures < 650 degreesC, initial cyclic hardening occurred, whereas > 650 degreesC a cyclic saturation state was observed from the beginning. With increasing temperature, fatigue life decreased in vacuum, but increased in air indicating an abnormal (inverse) environmental effect. The stress-strain behavior under TMF conditions resembles that of the corresponding isothermal experiments. Out-of-phase thermo-mechanical fatigue was found to be more detrimental than in-phase. because of the positive (tensile) mean stress arising in out-of-phase testing in combination with the pronounced mean stress sensitivity of the relatively brittle alloy. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:625 / 630
页数:6
相关论文
共 8 条
[1]  
FISCHER FOR, 1999, IN PRESS P 9 WORLD C
[2]  
FISCHER FOR, 1999, P WERKST 1998 OCT 12, P514
[3]   TENSION CREEP OF WROUGHT SINGLE-PHASE GAMMA-TIAL [J].
HAYES, RW ;
MARTIN, PL .
ACTA METALLURGICA ET MATERIALIA, 1995, 43 (07) :2761-2772
[4]   EFFECTS OF MICROSTRUCTURE ON THE DEFORMATION AND FRACTURE OF GAMMA-TIAL ALLOYS [J].
KIM, YW .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 192 :519-533
[5]   FUNDAMENTALS OF TIAL OXIDATION - A CRITICAL-REVIEW [J].
RAHMEL, A ;
QUADAKKERS, WJ ;
SCHUTZE, M .
WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1995, 46 (05) :271-285
[6]  
Skrotzki B, 1999, Z METALLKD, V90, P393
[7]  
Wagner R, 1995, GAMMA TITANIUM ALUMINIDES, P387
[8]   Effect of V and Nh addition on the fatigue behaviour of TiAl polysynthetically twinned crystals [J].
Yasuda, HY ;
Nakano, T ;
Nakazawa, J ;
Umakoshi, Y .
ISIJ INTERNATIONAL, 1997, 37 (12) :1210-1217