Effect of glazing application side and mechanical cycling on the biaxial flexural strength and Weibull characteristics of a Y-TZP ceramic

被引:9
|
作者
Martinelli Lobo, Carolina Machado [1 ]
Mota Cavalcanti Sacorague, Samia Carolina [1 ]
da Silva, Nathalia Ramos [2 ]
Figueiredo Costa, Anna Karina [1 ]
Martins Alves, Larissa Marcia [1 ]
Bottino, Marco Antonio [1 ]
Ozcan, Mutlu [3 ]
de Assuncao e Souza, Rodrigo Othavio [2 ]
de Melo, Renata Marques [1 ]
机构
[1] Univ Estadual Paulista, UNESP, Inst Ciencia & Tecnol, Dept Mat Dentarios & Protese, Sao Jose Dos Campos, SP, Brazil
[2] Univ Fed Rio Grande do Norte UFRN, Dept Odontol, Av Salgado Filho 1787, BR-59056000 Natal, RN, Brazil
[3] Univ Zurich, Ctr Dent & Oral Med, Dent Biomat, Clin Reconstruct Dent, Zurich, Switzerland
关键词
Ceramics; Dental stress analysis; Flexural Strength; Y-TZP; LITHIUM-DISILICATE; SURFACE TREATMENTS; FRACTURE STRENGTH; IN-VITRO; ZIRCONIA; CROWNS; RESISTANCE; PERFORMANCE; IMMEDIATE; SURVIVAL;
D O I
10.1590/1678-7757-2020-0438
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Glaze application on monolithic zirconia (Y-TZP) can be a practical approach to improve the mechanical properties of this material. Objective: Our study evaluated the effect of glazing side and mechanical cycling on the biaxial flexure strength (BFS) of a Y-TZP. Methodology: Eighty sintered Y-TZP discs (empty set:12 mm; thickness: 1.2 mm - ISO 6872) were produced and randomly assigned into eight groups (n=10), according to the factors "glazing side" (control - no glazing; GT - glaze on tensile side; GC - glaze on compression side; GTC - glaze on both sides) and "mechanical aging" (non -aged and aged, A - mechanical cycling: 1.2x106, 84 N, 3 Hz, under water at 37 degrees C). Specimens were subjected to BFS test (1 mm/min; 1,000 Kgf load cell) and fractured surfaces were analyzed by stereomicroscopy and SEM. Hsueh's rigorous solutions were used to estimate the stress at failure of glazed specimens. Two-way ANOVA, Tukey's test (5%), and Weibull analysis were performed. Results: The "glazing side", "mechanical aging" and the interaction of the factors were significant (p<0.05). Groups GC (1157.9 +/- 146.9 MPa), GT (1156.1 +/- 195.3 MPa), GTC (986.0 +/- 187.4 MPa) and GTC-A (1131.9 +/- 128.9 MPa) presented higher BFS than control groups (Tukey, 5%). Hsueh's rigorous solutions showed that the maximum tensile stress was presented in the bottom of zirconia layer, at the zirconia/glaze interface. Weibull characteristic strength (sigma(o)) of the GC was higher than all groups (p<0.05), except to GT, GTC-A and GTC, which were similar among them. The fractography showed initiation of failures from zirconia the tensile side regardless of the side of glaze application and fatigue. Conclusion: Glazing zirconia applied on both tensile and compression sides improves the flexural strength of Y-TZP, regardless the mechanical aging.
引用
收藏
页数:9
相关论文
共 37 条
  • [1] Effect of Surface and Heat Treatments on the Biaxial Flexural Strength and Phase Transformation of a Y-TZP Ceramic
    Fonseca, Renata Garcia
    Abi-Rached, Filipe de Oliveira
    Correia Pereira da Silva, Filipe Samuel
    Pacheco de Castro Henriques, Bruno Alexandre
    Pereira Pinelli, Ligia Antunes
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (05): : 451 - 458
  • [2] Flexural strength and Weibull analysis of Y-TZP fabricated by stereolithographic additive manufacturing and subtractive manufacturing
    Lu, Yuqing
    Mei, Ziyu
    Zhang, Junjing
    Gao, Shanshan
    Yang, Xingqiang
    Dong, Bo
    Yue, Li
    Yu, Haiyang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (03) : 826 - 834
  • [3] Biaxial flexural strength and Weibull characteristics of a resin ceramic material after thermal-cycling
    Beyabanaki, Elaheh
    Ashtiani, Reza Eftekhar
    Moradi, Mehrnoosh
    Namdari, Mahshid
    Mostafavi, Delaram
    Zandinejad, Amirali
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2023, 32 (08): : 721 - 727
  • [4] Effect of fatigue on biaxial flexural strength of bilayered porcelain/zirconia (Y-TZP) dental ceramics
    Yilmaz, Handan
    Nemli, Secil Karakoca
    Aydin, Cemal
    Bal, Bilge Turhan
    Tiras, Tulay
    DENTAL MATERIALS, 2011, 27 (08) : 786 - 795
  • [5] The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    Kosmac, T
    Oblak, C
    Jevnikar, P
    Funduk, N
    Marion, L
    DENTAL MATERIALS, 1999, 15 (06) : 426 - 433
  • [6] Thermo and mechanical cycling and veneering method do not influence Y-TZP core/veneer interface bond strength
    Vidotti, Hugo Alberto
    Pereira, Jefferson Ricardo
    Insaurralde, Elizeu
    Pompeia Fraga de Almeida, Ana Lucia
    do Valle, Accacio Lins
    JOURNAL OF DENTISTRY, 2013, 41 (04) : 307 - 312
  • [7] Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    Guazzato, M
    Quach, L
    Albakry, M
    Swain, MV
    JOURNAL OF DENTISTRY, 2005, 33 (01) : 9 - 18
  • [8] Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging
    Pereira, G. K. R.
    Silvestri, T.
    Camargo, R.
    Rippe, M. P.
    Amaral, M.
    Kleverlaan, C. J.
    Valandro, L. F.
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2016, 63 : 70 - 77
  • [9] EFFECT OF HIPING ON DEFECT AND STRENGTH CHARACTERISTICS IN Y-TZP
    KIM, JY
    UCHIDA, N
    UEMATSU, K
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1992, 100 (03): : 311 - 314
  • [10] Does the glaze application on Y-TZP surface improve the bond strength to pressed veneering ceramic?
    Rodrigues, Vinicius Aneas
    Paradella, Thais Cachute
    Coelho, Arianne Valim Pinto
    Souza, Karina Barbosa
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Ozcan, Mutlu
    Assuncao e Souza, Rodrigo Othavio
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (13) : 1459 - 1471