Hydrogen Transport in Tungsten for Nuclear Energy Application: Temperature Dependence and Compensation Effect

被引:4
作者
Yang, Kun Jie [1 ]
Liu, Yue-Lin [1 ]
Liu, Ning [1 ]
Shao, Peng [2 ]
Zhang, Xu [2 ]
Ma, Yuming [3 ]
机构
[1] Yantai Univ, Dept Nucl Engn & Technol, Yantai 264005, Peoples R China
[2] Harbin Inst Technol, Shenzhen Grad Sch, Shenzhen 518055, Peoples R China
[3] Paris Sud Univ, Dept Nucl Energy, F-91405 Orsay, France
基金
中国国家自然科学基金;
关键词
Tungsten; hydrogen transport; temperature and compensation effects; first principles; GENERALIZED GRADIENT APPROXIMATION; DIFFUSION CONSTANTS; DEUTERIUM RETENTION; 1ST WALL; 1ST-PRINCIPLES; METALS; CARBON; ATOMS;
D O I
10.1080/15361055.2020.1740556
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
We performed systematically first-principles calculations to investigate interstitial H diffusion/permeation of temperature dependence in tungsten (W). The interstitial H diffusion is primarily through two nearest-neighbor tetrahedral positions and its activation energy increases significantly with rising temperature. Phonon vibration plays a decisive role in the behavior of the H activation energy with rising temperature. The H permeation activation energy also depends strongly on the temperature since it is the sum of the formation energy and diffusion activation energy of H. Our calculated H diffusivity/permeability with the temperature agree quantitatively with the reliable experimental data within the error range in W. The vacancy-capturing effect can give a reasonable explanation of the discrepancy between simulation and experiment. Although the diffusion/permeation activation energy and the prefactor strongly depend on the temperature, the diffusivity/permeability of H still obeys quasi-Arrhenius behavior with rising temperature, which is attributed to the compensation effect between the activation energy and the prefactor, i.e., the increment of the prefactor compensates directly the modification of the diffusivity/permeability in the case of a variation in the activation energy with rising temperature.
引用
收藏
页码:616 / 631
页数:16
相关论文
共 85 条
[1]  
AITKEN EA, 1967, T METALL SOC AIME, V239, P1565
[2]   The effect of displacement damage on deuterium retention in ITER-grade tungsten exposed to low-energy, high-flux pure and helium-seeded deuterium plasmas [J].
Alimov, V. Kh. ;
Tyburska-Pueschel, B. ;
Hatano, Y. ;
Roth, J. ;
Isobe, K. ;
Matsuyama, M. ;
Yamanishi, T. .
JOURNAL OF NUCLEAR MATERIALS, 2012, 420 (1-3) :370-373
[3]   DEUTERIUM TRANSPORT AND TRAPPING IN POLYCRYSTALLINE TUNGSTEN [J].
ANDERL, RA ;
HOLLAND, DF ;
LONGHURST, GR ;
PAWELKO, RJ ;
TRYBUS, CL ;
SELLERS, CH .
FUSION TECHNOLOGY, 1992, 21 (02) :745-752
[4]  
[Anonymous], 1991, Atom movements, Diffusion and Mass Transport in solids
[5]  
[Anonymous], 1964, Ukr Fiz Zh
[6]   Hydrogen retention in high-Z materials with various contents of carbon [J].
Atsumi, H ;
Tanabe, T .
JOURNAL OF NUCLEAR MATERIALS, 1998, 258 :896-901
[7]   Hydrogen and deuterium transport and inventory parameters through W and W-alloys for fusion reactor applications [J].
Benamati, G ;
Serra, E ;
Wu, CH .
JOURNAL OF NUCLEAR MATERIALS, 2000, 283 :1033-1037
[8]   PROJECTOR AUGMENTED-WAVE METHOD [J].
BLOCHL, PE .
PHYSICAL REVIEW B, 1994, 50 (24) :17953-17979
[9]   First-Principles Study of Helium Trapping in Carbide Precipitates (Cr23C6) in Ferritic-Martensitic Steels [J].
Cao, Jin-Li ;
Xiao, Wei ;
Cao, Qi ;
He, Bing-Ling .
FUSION SCIENCE AND TECHNOLOGY, 2018, 74 (03) :177-185
[10]   Hydrogen isotope retention and recycling in fusion reactor plasma-facing components [J].
Causey, RA .
JOURNAL OF NUCLEAR MATERIALS, 2002, 300 (2-3) :91-117