Structural performance of ultra-high-performance concrete beams with different steel fibers

被引:381
作者
Yoo, Doo-Yeol [1 ]
Yoon, Young-Soo [2 ]
机构
[1] Univ British Columbia, Dept Civil Engn, Vancouver, BC V6T 1Z4, Canada
[2] Korea Univ, Sch Civil Environm & Architectural Engn, Seoul 136713, South Korea
关键词
Ultra-high-performance concrete; Flexure; Steel fiber; Ductility; Sectional analysis; Fiber orientation; SHRINKAGE-REDUCING ADMIXTURE; REINFORCED CONCRETE; FLEXURAL BEHAVIOR; COMPRESSIVE STRENGTH; SOFTENING CURVE; TENSILE;
D O I
10.1016/j.engstruct.2015.08.029
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this study, ten large ultra-high-performance concrete (UHPC) beams reinforced with steel rebars were fabricated and tested. The experimental parameters included reinforcement ratio and steel fiber type. Two different reinforcement ratios (rho = 0.94% and 1.50%) and steel fiber types (smooth and twisted steel fibers) were adopted. In addition, three different fiber lengths (L-f = 13, 19.5, and 30 mm) for the smooth steel fibers and one fiber length (L-f = 30 mm) for the twisted steel fiber were considered. For a control specimen, a UHPC matrix without fiber was also considered. Test results indicated that the addition of steel fibers significantly improved the load carrying capacity, post-cracking stiffness, and cracking response, but it decreased the ductility. Specifically, with the inclusion of 2% by volume of steel fibers, approximately 27-54% higher load carrying capacity and 13-73% lower ductility were obtained. In addition, an increase in the length of smooth steel fibers and the use of twisted steel fibers led to the improvements of post-peak response and ductility, whereas no noticeable difference in the load carrying capacity, post-cracking stiffness, and cracking response were obtained according to the fiber length and type. Sectional analysis incorporating the suggested material models was also performed based on AFGC/SETRA recommendations, and the ratios of flexural capacities obtained from experiments and numerical analyses ranged from 0.91 to 1.19. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:409 / 423
页数:15
相关论文
共 47 条
[1]  
[Anonymous], 2003, JCI-S-002-2003
[2]  
[Anonymous], 2008, P 4 INT IABMAS C
[3]  
[Anonymous], 2022, Astm C78/C78M-22, P1, DOI [DOI 10.1520/C0078, 10.1520/C0078_C0078M-22]
[4]  
[Anonymous], 2007, DIANA USERS MANUAL R
[5]  
[Anonymous], 2016, Annu. B. ASTM Stand, DOI [10.1520/C0157, DOI 10.1520/C0157]
[6]  
Aoude H, 2012, ACI STRUCT J, V109, P359
[7]  
Association Francaise de Genie (AFGC), 2002, ULTR PERF FIBR REINF
[8]   Response of normal-strength and ultra-high-performance fiber-reinforced concrete columns to idealized blast loads [J].
Astarlioglu, Serdar ;
Krauthammer, Ted .
ENGINEERING STRUCTURES, 2014, 61 :1-12
[9]   The effect of fiber properties on high performance alkali-activated slag/silica fume mortars [J].
Aydin, Serdar ;
Baradan, Bulent .
COMPOSITES PART B-ENGINEERING, 2013, 45 (01) :63-69
[10]   Assessment of fibre orientation in ultra high performance fibre reinforced concrete and its effect on flexural strength [J].
Barnett, Stephanie J. ;
Lataste, Jean-Francois ;
Parry, Tony ;
Millard, Steve G. ;
Soutsos, Marios N. .
MATERIALS AND STRUCTURES, 2010, 43 (07) :1009-1023