Radiographic inspection of porosity in Ti-6Al-4V laser-welded joints

被引:3
作者
Costa Nunez-Pantoja, Juliana Maria [1 ]
Ferreira Koyama Takahashi, Jessica Mie [1 ]
de Arruda Nobilo, Mauro Antonio [1 ]
Xediek Consani, Rafael Leonardo [1 ]
Mesquita, Marcelo Ferraz [1 ]
机构
[1] Univ Estadual Campinas, Piracicaba Dent Sch, Dept Prosthodont & Periodontol, Piracicaba, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Titanium; Dental Soldering; Radiography; Dental; Dental Alloys; COMMERCIALLY PURE TITANIUM; MECHANICAL-PROPERTIES; ALLOY; CAST; STRENGTH; FATIGUE;
D O I
10.1590/S1806-83242011005000005
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Widely used in dentistry, Ti-6Al-4V alloy is difficult to cast and solder, as it frequently exhibits pores inside the structure. This study was conducted to evaluate the effect of joint openings and diameters of laser-welded joints executed in Ti-6Al-4V structures on the presence of pores as checked by radiographic procedures. Sixty dumbbell rods with central diameters of 1.5, 2.0 and 3.5 mm were created from Ti-6Al-4V-wrought bars. Specimens were sectioned and welded using two joint openings (0.0 and 0.6 mm). The combination of variables created six groups (n = 10). Laser welding was executed using 360V/8ms (1.5 and 2.0 mm) and 380V/9ms (3.5 mm), with the focus and frequency set to zero. The joints were finished, polished and submitted to radiographic examination. The radiographs were visually examined for the presence of pores in the joints, qualitatively. The percentage of radiographic presence of pores was calculated without counting pores per joint. Data were analyzed using a chi-square test (alpha = 0.05). For the 1.5-mm specimens, the incidence of pore presence was significantly higher (p = 0.0001) when using 0.6-mm joint openings (40%) compared to 0.0-mm openings (0%). For the 2.0-mm specimens, there was no significant difference between groups (p = 0.2008). However, for the 3.5-mm specimens, the incidence of pore presence was lower (p = 0.0061) for 0.6-mm openings (50%) compared to 0.0-mm openings (70%). Therefore, laser welding of Ti-6Al-4V structures with thin diameters provides the best condition for the juxtaposition of the parts.
引用
收藏
页码:103 / 108
页数:6
相关论文
共 50 条
  • [1] Beta grain size evolution in laser-welded Ti-6Al-4V
    Patterson, T.
    Lippold, J.
    Panton, B.
    WELDING IN THE WORLD, 2022, 66 (11) : 2231 - 2243
  • [2] Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers
    Hosseini, Seyed Reza Elmi
    Feng, Kai
    Nie, Pulin
    Zhang, Ke
    Huang, Jian
    Li, Zhuguo
    Kokawa, Hiroyuki
    Guo, Baochao
    Xue, Song
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (11) : 6135 - 6148
  • [3] Superplastic deformation mechanism and mechanical behavior of a laser-welded Ti-6Al-4V alloy joint
    Chen, Shuhai
    Huang, Jihua
    Cheng, Donghai
    Zhang, Hua
    Zhao, Xingke
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 541 : 110 - 119
  • [4] A study on the role of local residual stress on the local strength and defect growth in laser-welded Ti-6Al-4V
    Sun, Wei
    Xia, Yiping
    Chen, Min
    Fan, Guohua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1018
  • [5] Microstructure and mechanical properties of laser welded lap joints of Ti-6Al-4V alloy
    Zhao, Yong
    Huang, Jian
    Zhao, Ying
    Wu, Yixiong
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 2375 - 2378
  • [6] Distribution of Al Element of Ti-6Al-4V Joints by Fiber Laser Welding
    Zhang, Jiajia
    Hu, Renzhi
    Pang, Shengyong
    Huang, Anguo
    COATINGS, 2019, 9 (09)
  • [7] Effect of welding parameters on morphology and mechanical properties of Ti-6Al-4V laser beam welded butt joints
    Squillace, A.
    Prisco, U.
    Ciliberto, S.
    Astarita, A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2012, 212 (02) : 427 - 436
  • [8] Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers
    Seyed Reza Elmi Hosseini
    Kai Feng
    Pulin Nie
    Ke Zhang
    Jian Huang
    Zhuguo Li
    Hiroyuki Kokawa
    Baochao Guo
    Song Xue
    Journal of Materials Engineering and Performance, 2018, 27 : 6135 - 6148
  • [9] A study of fatigue damage evolution on pulsed Nd:YAG Ti6Al4V laser welded joints
    Liu, Jing
    Gao, Xiao-Long
    Zhang, Lin-Jie
    Zhang, Jian-Xun
    ENGINEERING FRACTURE MECHANICS, 2014, 117 : 84 - 93
  • [10] Forming and tensile fracture characteristics of Ti-6Al-4V and T2 Cu vacuum electron beam welded joints
    Guo, Shun
    Peng, Yong
    Cui, Chong
    Zhou, Qi
    Xu, Junqiang
    Zhu, Jun
    VACUUM, 2019, 165 (311-319) : 311 - 319