Evolution of surface chemistry and morphology of oxide scale formed during initial stage oxidation of modified 9Cr-1Mo steel

被引:52
作者
Swaminathan, Srinivasan [1 ]
Mallika, C. [1 ]
Krishna, Nanda Gopala [1 ]
Thinaharan, C. [1 ]
Jayakumar, T. [1 ]
Mudali, U. Kamachi [1 ]
机构
[1] Indira Gandhi Ctr Atom Res, Met & Mat Grp, Kalpakkam 603102, Tamil Nadu, India
关键词
Alloy; Steel; XPS; SEM; Segregation; Oxidation; FERRITIC-MARTENSITIC STEELS; CYCLE FATIGUE BEHAVIOR; SELECTIVE OXIDATION; CORROSION BEHAVIOR; WATER-VAPOR; TEMPERATURE; CREEP; T91; CR; RESISTANCE;
D O I
10.1016/j.corsci.2013.10.026
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Initial stage oxidation characteristics of the modified 9Cr-1Mo steel in ambient air at 650 degrees C have been investigated, for exposure times ranging from 5 to 500 h. Oxygen flux from the gas phase causes high initial oxidation rate, but the growth kinetics do not follow parabolic law. In "as-received" condition, binary oxides of Fe and Cr were found as native oxides. Upon oxidation, segregation of Mn resulted in the formation of MnCr2O4 along with FeCr2O4 and binary oxides of Fe, Cr and Mn. Thus, the initial oxide scale constitutes multiple oxides with delineated interface, unlikely to have a layered structure. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:59 / 68
页数:10
相关论文
共 41 条
  • [11] Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: A synthesis of current understanding
    Guzonas, D. A.
    Cook, W. G.
    [J]. CORROSION SCIENCE, 2012, 65 : 48 - 66
  • [12] High Temperature Materials for Nuclear Fast Fission and Fusion Reactors and Advanced Fossil Power Plants
    Jayakumar, T.
    Mathew, M. D.
    Laha, K.
    [J]. 6TH INTERNATIONAL CONFERENCE ON CREEP, FATIGUE AND CREEP-FATIGUE INTERACTION, 2013, 55 : 259 - 270
  • [13] Oxidation of Fe-10Cr in O2 and in O2+H2O environment at 600 °C: A microstructural investigation
    Jonsson, T.
    Pujilaksono, B.
    Heidari, H.
    Liu, F.
    Svensson, J. -E.
    Halvarsson, M.
    Johansson, L-G.
    [J]. CORROSION SCIENCE, 2013, 75 : 326 - 336
  • [14] Ferritic/martensitic steels for next-generation reactors
    Klueh, R. L.
    Nelson, A. T.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2007, 371 (1-3) : 37 - 52
  • [15] CHROMIUM MOLYBDENUM STEELS FOR FUSION-REACTOR 1ST WALLS - A REVIEW
    KLUEH, RL
    [J]. NUCLEAR ENGINEERING AND DESIGN, 1982, 72 (03) : 329 - 344
  • [16] KLUEH RL, 1992, J NUCL MATER, V191, P116
  • [17] Kofstad P., 1988, HIGH TEMPERATURE COR
  • [18] Lai G.Y., 2007, High Temperature Corrosion and Materials Applications
  • [19] Continuous and cyclic oxidation of T91 ferritic steel under steam
    Laverde, D
    Gómez-Acebo, T
    Castro, F
    [J]. CORROSION SCIENCE, 2004, 46 (03) : 613 - 631
  • [20] Lince J.R., 1992, TR92293510 AER CORP