Evolution of surface chemistry and morphology of oxide scale formed during initial stage oxidation of modified 9Cr-1Mo steel

被引:52
作者
Swaminathan, Srinivasan [1 ]
Mallika, C. [1 ]
Krishna, Nanda Gopala [1 ]
Thinaharan, C. [1 ]
Jayakumar, T. [1 ]
Mudali, U. Kamachi [1 ]
机构
[1] Indira Gandhi Ctr Atom Res, Met & Mat Grp, Kalpakkam 603102, Tamil Nadu, India
关键词
Alloy; Steel; XPS; SEM; Segregation; Oxidation; FERRITIC-MARTENSITIC STEELS; CYCLE FATIGUE BEHAVIOR; SELECTIVE OXIDATION; CORROSION BEHAVIOR; WATER-VAPOR; TEMPERATURE; CREEP; T91; CR; RESISTANCE;
D O I
10.1016/j.corsci.2013.10.026
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Initial stage oxidation characteristics of the modified 9Cr-1Mo steel in ambient air at 650 degrees C have been investigated, for exposure times ranging from 5 to 500 h. Oxygen flux from the gas phase causes high initial oxidation rate, but the growth kinetics do not follow parabolic law. In "as-received" condition, binary oxides of Fe and Cr were found as native oxides. Upon oxidation, segregation of Mn resulted in the formation of MnCr2O4 along with FeCr2O4 and binary oxides of Fe, Cr and Mn. Thus, the initial oxide scale constitutes multiple oxides with delineated interface, unlikely to have a layered structure. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:59 / 68
页数:10
相关论文
共 41 条
  • [1] Abe F, 2008, WOODHEAD PUBL MATER, P1, DOI 10.1533/9781845694012
  • [2] Oxidation of ferritic-martensitic alloys T91, HCM12A and HT-9 in supercritical water
    Ampornrat, Pantip
    Was, Gary S.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2007, 371 (1-3) : 1 - 17
  • [3] Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni
    Biesinger, Mark C.
    Payne, Brad P.
    Grosvenor, Andrew P.
    Lau, Leo W. M.
    Gerson, Andrea R.
    Smart, Roger St. C.
    [J]. APPLIED SURFACE SCIENCE, 2011, 257 (07) : 2717 - 2730
  • [4] Corrosion behavior of ferritic-martensitic steel T91 in supercritical water
    Chen, Yun
    Sridharan, Kumar
    Allen, Todd
    [J]. CORROSION SCIENCE, 2006, 48 (09) : 2843 - 2854
  • [5] Prediction of the depletion zone due to selective oxidation of P91 steel
    Danielewski, M
    Filipek, R
    Kucharska, B
    [J]. DIFFUSION IN MATERIALS: DIMAT 2004, PTS 1 AND 2, 2005, 237-240 : 965 - 970
  • [6] EFFECT OF PROCESSING ON THE HIGH-TEMPERATURE LOW-CYCLE FATIGUE PROPERTIES OF MODIFIED 9CR-1MO FERRITIC STEEL
    EBI, G
    MCEVILY, AJ
    [J]. FATIGUE OF ENGINEERING MATERIALS AND STRUCTURES, 1984, 7 (04): : 299 - 314
  • [7] Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments
    Ehlers, J.
    Young, D. J.
    Smaardijk, E. J.
    Tyagi, A. K.
    Penkalla, H. J.
    Singheiser, L.
    Quadakkers, W. J.
    [J]. CORROSION SCIENCE, 2006, 48 (11) : 3428 - 3454
  • [8] Faulkner RG, 2008, WOODHEAD PUBL MATER, P329, DOI 10.1533/9781845694012.2.329
  • [9] Fry A., 2002, OXIDATION ALLOYS STE
  • [10] The oxidation of industrial FeCrMo steel
    Greeff, AP
    Louw, CW
    Swart, HC
    [J]. CORROSION SCIENCE, 2000, 42 (10) : 1725 - 1740