Hydrogen diffusion and trapping in a precipitation-hardened nickel-copper-aluminum alloy Monel K-500 (UNS N05500)

被引:55
作者
Ai, Jia-He [1 ]
Ha, Hung M. [1 ]
Gangloff, Richard P. [1 ]
Scully, John R. [1 ]
机构
[1] Univ Virginia, Dept Mat Sci & Engn, Ctr Electrochem Sci & Engn, Charlottesville, VA 22904 USA
关键词
Age hardening; Nickel alloy; Hydrogen diffusion and trapping; Hydrogen embrittlement; Hydrogen desorption; NI-CU; ASSISTED CRACKING; GRAIN-BOUNDARIES; EMBRITTLEMENT; SOLUBILITY; CO; TEMPERATURE; TRANSPORT; FORMULA; METALS;
D O I
10.1016/j.actamat.2013.02.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen uptake, diffusivity and trap binding energy were determined for the nickel-copper-aluminum alloy Monel K-500 (UNS N05500) in several conditions. The total atomic hydrogen (H) concentration increased from 0 to 132 wppm as the hydrogen overpotential decreased to -0.5 V in alkaline 3.5% NaCl electrolyte at 23 degrees C. The room-temperature H diffusion coefficient ranged from 0.9 to 3.9 x 10(-14) m(2) s(-1) for single-phase solid solution, aged, and cold worked then aged microstructures. Diffusivity was independent of lattice H concentration but depended weakly on metallurgical condition, with slower H diffusion after aging. The apparent activation energy for H diffusion was in the range of 29-41 +/- 1.5 kJ mol(-1) at the 95% confidence level. The lower value approached nearly perfect lattice transport, while the high value was strongly influenced by traps of low-to-intermediate strength. Atomic hydrogen trapping at metallurgical sites, strongly suggested to be spherical-coherent gamma' (Ni3Al) precipitates, was evident in the aged compared to the solution heat treated + water-quenched condition. Both thermal desorption and classical Oriani trap state analyses confirmed that the apparent hydrogen trap binding energy interpreted as Ni3Al (10.2 +/- 4.6 kJ mol(-1)) interfaces was significantly less than the activation energy for perfect lattice diffusion (25.6 +/- 0.5 kJ mol-1) in this nickel-based alloy system. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3186 / 3199
页数:14
相关论文
共 62 条
  • [1] Alefeld G., 1978, HYDROGEN METALS BASI
  • [2] TRAPPING OF HYDROGEN TO LATTICE-DEFECTS IN NICKEL
    ANGELO, JE
    MOODY, NR
    BASKES, MI
    [J]. MODELLING AND SIMULATION IN MATERIALS SCIENCE AND ENGINEERING, 1995, 3 (03) : 289 - 307
  • [3] [Anonymous], 2000, QQN286G HIS
  • [4] ON MODULATED STRUCTURE OF AGED NI-AL ALLOYS
    ARDELL, AJ
    NICHOLSO.RB
    [J]. ACTA METALLURGICA, 1966, 14 (10): : 1295 - +
  • [5] ASTM, 2005, STAND TEST METH EL M
  • [6] HYDROGEN TRAPPING PHENOMENA IN CARBON-STEEL
    CHOO, WY
    LEE, JY
    [J]. JOURNAL OF MATERIALS SCIENCE, 1982, 17 (07) : 1930 - 1938
  • [7] THERMAL-ANALYSIS OF TRAPPED HYDROGEN IN PURE IRON
    CHOO, WY
    LEE, JY
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (01): : 135 - 140
  • [8] Copson HR, 1956, CORROSION, V12, P647
  • [9] Crank J., 1975, The Mathematics of Diffusion, V2nd
  • [10] Deluccia J.J., 1981, Electrochemical Corrosion Testing, ASTM STP 727, P256