Improved High Temperature Performance of a Spinel LiNi0.5Mn1.5O4 Cathode for High-Voltage Lithium-Ion Batteries by Surface Modification of a Flexible Conductive Nanolayer

被引:39
作者
Dong, Hongyu [1 ,2 ,3 ]
Zhang, Yijia [1 ,2 ,3 ]
Zhang, Shiquan [1 ,2 ,3 ]
Tang, Panpan [1 ,2 ,3 ]
Xiao, Xinglu [1 ,2 ,3 ]
Ma, Mengyue [3 ,4 ]
Zhang, Huishuang [1 ,2 ,3 ]
Yin, Yanhong [1 ,2 ,3 ]
Wang, Dong [1 ,2 ]
Yang, Shuting [1 ,2 ,3 ]
机构
[1] Henan Normal Univ, Coll Chem & Chem Engn, Construct East Rd, Xinxiang 453007, Henan, Peoples R China
[2] Henan Normal Univ, Natl & Local Engn Lab Motive Power & Key Mat, Construct East Rd, Xinxiang 453007, Henan, Peoples R China
[3] Henan Normal Univ, Collaborat Innovat Ctr Henan Prov Motive Power &, Construct East Rd, Xinxiang 453007, Henan, Peoples R China
[4] Henan Normal Univ, Henan Battery Res Inst, Construct East Rd, Xinxiang 453007, Henan, Peoples R China
来源
ACS OMEGA | 2019年 / 4卷 / 01期
基金
中国国家自然科学基金;
关键词
SOLID-ELECTROLYTE INTERFACE; ELECTROCHEMICAL-BEHAVIOR; CYCLING STABILITY; RATE CAPABILITY; LI; CAPACITY; ENERGY; LIMN1.5NI0.5O4; CHALLENGES; DEPOSITION;
D O I
10.1021/acsomega.8b02571
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The composite cathode material of the conductive polymer polyaniline (PANI)-coated spinel structural LiNi0.5Mn1.5O4 (LNMO) for high-voltage lithium-ion batteries has been successfully synthesized by an in situ chemical oxidation polymerization method. The electrode of the LNMO-PANI composite material shows superior rate capability and excellent cycling stability. A capacity of 123.4 mAh g(-1) with the capacity retention of 99.7% can be maintained at 0.5C after 200 cycles in the voltage range of 3.0-4.95 V (vs Li/Li+) at room temperature. Even with cycling at 5C, a capacity of 65.5 mAh g(-1) can still be achieved. The PANI coating layer can not only reduce the dissolution of Ni and Mn from the LNMO cubic framework into the electrolyte during cycling, but also significantly improve the undesirable interfacial reactions between the cathode and electrolyte, and markedly increase the electrical conductivity of the electrode. At 55 degrees C, the LNMO-PANI composite material exhibits more superior cyclic performance than pristine, that is, the capacity retention of 94.5% at 0.5C after 100 cycles vs that of 13.0%. This study offers an effective strategy for suppressing the decomposition of an electrolyte under the highly oxidizing (> 4.5 V) and elevated temperature conditions.
引用
收藏
页码:185 / 194
页数:10
相关论文
共 47 条
  • [31] Understanding Transition-Metal Dissolution Behavior in LiNi0.5Mn1.5O4 High-Voltage Spinel for Lithium Ion Batteries
    Pieczonka, Nicholas P. W.
    Liu, Zhongyi
    Lu, Peng
    Olson, Keith L.
    Moote, John
    Powell, Bob R.
    Kim, Jung-Hyun
    [J]. JOURNAL OF PHYSICAL CHEMISTRY C, 2013, 117 (31) : 15947 - 15957
  • [32] Enhanced electrochemical properties of ZnO-coated LiMnPO4 cathode materials for lithium ion batteries
    Rajammal, K.
    Sivakumar, D.
    Duraisamy, Navaneethan
    Ramesh, K.
    Ramesh, S.
    [J]. IONICS, 2016, 22 (09) : 1551 - 1556
  • [33] Studies on electrochemical behaviour of zinc-doped LiFePO4 for lithium battery positive electrode
    Shenouda, Atef Y.
    Liu, Hua K.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 477 (1-2) : 498 - 503
  • [34] Electrochemical behaviour of tin borophosphate negative electrodes for energy storage systems
    Shenouda, Atef Y.
    Liu, Hua Kun
    [J]. JOURNAL OF POWER SOURCES, 2008, 185 (02) : 1386 - 1391
  • [35] Defect Formation Energy in Spinel LiNi0.5Mn1.5O4-δ Using Ab Initio DFT Calculations
    Shiiba, Hiromasa
    Zettsu, Nobuyuki
    Nakayama, Masanobu
    Oishi, Shuji
    Teshima, Katsuya
    [J]. JOURNAL OF PHYSICAL CHEMISTRY C, 2015, 119 (17) : 9117 - 9124
  • [36] Simultaneous fluorination of active material and conductive agent for improving the electrochemical performance of LiNi0.5Mn1.5O4 electrode for lithium-ion batteries
    Song, Min Sang
    Kim, Dae Sik
    Park, Eunjun
    Choi, Jae Man
    Kim, Hansu
    [J]. JOURNAL OF POWER SOURCES, 2016, 326 : 156 - 161
  • [37] Investigation of the Solid Electrolyte Interphase Formation at Graphite Anodes in Lithium-Ion Batteries with Electrochemical Impedance Spectroscopy
    Steinhauer, Miriam
    Risse, Sebastian
    Wagner, Norbert
    Friedrich, K. Andreas
    [J]. ELECTROCHIMICA ACTA, 2017, 228 : 652 - 658
  • [38] Significant improvement in performances of LiNi0.5Mn1.5O4 through surface modification with high ordered Al-doped ZnO electro-conductive layer
    Sun, Hongdan
    Xia, Bingbo
    Liu, Weiwei
    Fang, Guoqing
    Wu, Jingjing
    Wang, Haibo
    Zhang, Ruixue
    Kaneko, Shingo
    Zheng, Junwei
    Wang, Hongyu
    Li, Decheng
    [J]. APPLIED SURFACE SCIENCE, 2015, 331 : 309 - 314
  • [39] Key challenges in future Li-battery research
    Tarascon, J. -M.
    [J]. PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 2010, 368 (1923): : 3227 - 3241
  • [40] Improving the electrochemical performances of spherical LiNi0.5Mn1.5O4 by Fe2O3 surface coating for lithium-ion batteries
    Wang, Gang
    Wen, Weicheng
    Chen, Shuhua
    Yu, Ruizhi
    Wang, Xianyou
    Yang, Xiukang
    [J]. ELECTROCHIMICA ACTA, 2016, 212 : 791 - 799