共 63 条
Temperature-induced and crystallization-driven self-assembly of polyethylene-b-poly(ethylene oxide) in solution
被引:62
作者:
Li, ZhiYun
[1
]
Liu, Ran
[1
]
Mai, BiYun
[1
]
Wang, WanJuan
[1
]
Wu, Qing
[1
,2
]
Liang, GuoDong
[1
,2
]
Gao, HaiYang
[1
,2
]
Zhu, FangMing
[1
,2
]
机构:
[1] Sun Yat Sen Univ, Sch Chem & Chem Engn, Minist Educ, Key Lab Polymer Composite & Funct Mat, Guangzhou 510275, Guangdong, Peoples R China
[2] Sun Yat Sen Univ, Sch Chem & Chem Engn, Inst Polymer Sci, DSAPM Lab, Guangzhou 510275, Guangdong, Peoples R China
来源:
基金:
中国国家自然科学基金;
关键词:
Linear polyethylene;
Block copolymer;
Self-assembly;
SEMICRYSTALLINE BLOCK-COPOLYMERS;
COIL DIBLOCK COPOLYMER;
SELECTIVE SOLVENT;
AQUEOUS-SOLUTION;
DILUTE-SOLUTION;
CYLINDRICAL MICELLES;
LINEAR POLYETHYLENE;
LIGHT-SCATTERING;
CHAIN;
TRANSITION;
D O I:
10.1016/j.polymer.2013.01.044
中图分类号:
O63 [高分子化学(高聚物)];
学科分类号:
070305 ;
080501 ;
081704 ;
摘要:
In this paper, the well-defined diblock copolymers consisting a linear polyethylene (LPE) and a poly (ethylene oxide) (PEO), LPE-b-PEO, were synthesized by combining the ethylene living coordination polymerization with fluorinated bis(phenoxyimine) titanium catalyst and the living ring-opening polymerization of ethylene oxide initiated by hydroxyl-terminated polyethylene (LPE OH) as a macromolecular initiator. We describe two methodologies for the self-assembly of LPE-b-PEO, namely temperature-induced self-assembly and crystallization-driven self-assembly. Transmission electron microscopy (TEM), atomic force microscopy (AFM) and dynamic light scattering (DLS) are employed to characterize the morphology, structure and hydrodynamic radius (R-h) of the self-assembled micelles. LPE-b-PEO is dissolved to form a molecular solution in trichlorobenzene (TCB) at 140 degrees C, while self-assembly could be driven when the crystallization of LPE blocks is induced by cooling to form diamond-shaped micelles with a mono-layer crystallized LPE lamella core. The resultant diblock copolymers can self-assemble into spherical micelles composed of a molten LPE core and a soluble PEO corona in DMF at 140 degrees C, that is above the melting temperature (T-m) of the LPE block. As the temperature decrease, the morphology changes from spherical to platelet-like micelle with a double-layer crystallized LPE lamella core sandwiched by solvent-swollen PEO corona. Furthermore, the confined crystallization of LPE block in nanosized self-assembled micelle core is investigated by differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (WAXRD). (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1663 / 1670
页数:8
相关论文