Development of adhesive bonds with reduced fracture strength as NDE benchmarks

被引:4
|
作者
Jastrzebski, M. U. [1 ]
Sinclair, A. N. [1 ]
Raizenne, D. D. [2 ]
Spelt, J. K. [1 ]
机构
[1] Univ Toronto, Toronto, ON M5S 3G8, Canada
[2] Natl Res Council Canada, Inst Aerosp Res, Ottawa, ON K1A 0R6, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Epoxy/epoxides; Aluminum and alloys; Durability non-destructive testing; JOINTS; DEGRADATION; ALUMINUM; FAILURE;
D O I
10.1016/j.ijadhadh.2008.07.004
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
A method for producing adhesively bonded aluminum joints with a predictable loss of fracture strength was developed and evaluated. The method uses an open-faced specimen geometry and a humid high-temperature environment to promote adhesive degradation. The rate of degradation was greatly increased over previous accelerated degradation schemes through the Use Of MgSO4 as a contaminant. The contaminant was applied as an aerosol in a purpose-built duct having a controlled airflow. Specimens were prepared and subjected to accelerated aging under a variety of conditions and then fractured using a DCB loading jig. It was found that the contaminant surface concentration was a strong determinant of the fracture strength after hot-wet aging. Exposure to the hot-wet environment was shown to have little effect beyond an initial threshold. Standard ultrasonic imaging techniques were incapable of differentiating between fresh and hot-wet aged specimens, in spite of significant differences in the fracture strength. This is consistent with the hypothesis that the approach produced specimens that simulated the effects of environmental attack, since standard ultrasonic methods, such as those used in the present study, cannot detect such losses of fracture strength in the absence of any delamination between adhesive and adherend. FESEM and EDX analysis of the fracture surfaces showed residual aluminum, suggesting an intra-oxide locus of failure consistent with other accelerated degradation methods. The technique can be used to generate adhesive joint specimens to aid the development of ultrasonic methods capable of detecting the loss of fracture strength associated with environmental degradation. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:372 / 379
页数:8
相关论文
共 50 条
  • [21] Ultrasonic Pulse-Echo NDE of Adhesive Bonds in Sheet-Metal Assemblies
    Chapman, G. B.
    Sadler, J.
    Maev, R. G.
    Titov, S.
    Maeva, E. Y.
    Severina, I.
    Severin, F.
    2006 IEEE ULTRASONICS SYMPOSIUM, VOLS 1-5, PROCEEDINGS, 2006, : 906 - 909
  • [22] Formation and fracture of adhesive bonds between colloidal spheres
    Stainton, C
    Liang, W
    Kendall, K
    ENGINEERING FRACTURE MECHANICS, 1998, 61 (01) : 83 - 91
  • [23] Fracture behaviour of adhesive bonds by different shear speed
    Paproth, A.
    Walter, S.
    Wolter, K. -J.
    58TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE, PROCEEDINGS, 2008, : 1679 - 1683
  • [24] THE FRACTURE-BEHAVIOR OF POLYMER METAL ADHESIVE BONDS
    TING, RY
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1982, 184 (SEP): : 81 - ORPL
  • [25] Comparison of variables influence on adhesive bonds strength calculations
    Müller, M. (muller@tf.czu.cz), 1600, Jan-Evangelista-Purkyne-University (13):
  • [26] ULTRASONIC ANALYSIS OF NONLINEAR RESPONSE AND STRENGTH OF ADHESIVE BONDS
    ACHENBACH, JD
    PARIKH, OK
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1991, 5 (08) : 601 - 618
  • [27] Influence of Adhesive Film Thickness on the Strength of Bonds.
    Schlimmer, Michael
    1600, (31):
  • [28] INFLUENCE OF OVERLAPPING LENGTH ON PEELING STRENGTH OF ADHESIVE BONDS
    Cidlina, Jan
    Muller, Miroslav
    14TH INTERNATIONAL SCIENTIFIC CONFERENCE: ENGINEERING FOR RURAL DEVELOPMENT, 2015, : 761 - 765
  • [30] EFFECT OF ENVIRONMENTAL DEGRADATION ON THE ADHESIVE BONDS STRENGTH AND DURABILITY
    Cidlina, Jan
    Henc, Petr
    TRENDS IN AGRICULTURAL ENGINEERING 2013, 2013, : 685 - 689