Cooling rate and microstructure of rapidly solidified Al-20 wt.% Si alloy

被引:93
|
作者
Xu, CL [1 ]
Wang, HY [1 ]
Qiu, F [1 ]
Yang, YF [1 ]
Jiang, QC [1 ]
机构
[1] Jilin Univ, Dept Mat Sci & Engn, Minist Educ, Key Lab Automobile Mat, Changchun 130025, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2006年 / 417卷 / 1-2期
基金
中国国家自然科学基金;
关键词
melt-spun ribbon; temperature distribution; cooling rate; Al-Si alloys;
D O I
10.1016/j.msea.2005.10.040
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A 40 mu m thick melt-spun ribbon was manufactured by using a single roller melt-spinning technique, and the temperature distribution of the melt-spun ribbon was obtained. The solidification time and the cooling rate of the melt-spun ribbon were estimated to be 6.59 x 10(-5) s and 1.11 X 10(6) degrees C/s, respectively. The morphologies of primary silicon in the melt-spun ribbon were drastically changed to fine block-shape (maximum size of primary silicon is 5 mu m, minimum size of primary silicon is 0.5 mu m and average size of primary silicon is 2 mu m), and the smaller eutectic silicon can be obtained due to the rapid solidification. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:275 / 280
页数:6
相关论文
共 50 条
  • [41] EVOLUTION OF MICROSTRUCTURE IN A RAPIDLY SOLIDIFIED AL-FE-V-SI ALLOY
    PARK, WJ
    AHN, S
    KIM, NJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 189 (1-2): : 291 - 299
  • [42] Microstructure characteristics of a rapidly solidified Al-Si-Ti-Pb alloy
    Tong, XC
    Fang, HS
    MATERIALS CHARACTERIZATION, 1996, 37 (2-3) : 95 - 104
  • [43] Effect of ultrasonic treatment and Sr addition on microstructure of Al-20%Si alloy
    Miao Long
    Lu Yiping
    Zhang Yubo
    Fu Ying
    Li Tingju
    China Foundry, 2013, (04) : 213 - 216
  • [44] Effect of ultrasonic treatment and Sr addition on microstructure of Al-20%Si alloy
    Miao Long
    Lu Yiping
    Zhang Yubo
    Fu Ying
    Li Tingju
    CHINA FOUNDRY, 2013, 10 (04) : 213 - 216
  • [45] Effect of ultrasonic treatment and Sr addition on microstructure of Al-20%Si alloy
    Miao Long
    Lu Yiping
    Zhang Yubo
    Fu Ying
    Li Tingju
    China Foundry, 2013, 10 (04) : 213 - 216
  • [46] Microstructure evolution of Al-20%Si alloy with ultrasonic standing wave treatment
    Wang, Hong-Ling
    Le, Qi-Chi
    Zhang, Zhi-Qiang
    Cui, Jian-Zhong
    Zhang, Xiang-Wen
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2014, 24 (11): : 2749 - 2754
  • [47] Effect of cooling rate on the microstructure of rapidly solidified SiGe
    Hussain, Naveed
    Mullis, Andrew M.
    Haque, Nafisul
    MATERIALS CHARACTERIZATION, 2019, 154 : 377 - 385
  • [48] Study on behaviors of annealed microstructure developed in rapidly solidified Al-20Si-5Fe alloy
    Chen, Yiqing
    Su, Yong
    Ding, Houfu
    Huang, Xinmin
    Zheng, Yuchun
    Jinshu Rechuli Xuebao/Transactions of Metal Heat Treatment, 2000, 21 (03): : 46 - 50
  • [49] Section-dependent microstructure and mechanical properties of rapidly solidified and extruded Al-20Si alloy
    Hong, SJ
    Suryanarayana, C
    Chun, BS
    MATERIALS RESEARCH BULLETIN, 2004, 39 (03) : 465 - 474
  • [50] Formation of hypoeutectic microstructure in a rapidly solidified Al-5 wt-%Sr alloy
    Zhang, ZH
    Bian, XF
    Wang, Y
    MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (06) : 791 - 795